Reflection high-energy electron diffraction is a Bragg case, in which the beams to be detected are those reflected from the bulk crystal surface. Owing to the strong interaction between the incident electron and the crystal atoms, multiple (or dynamical) scattering is very strong. Although the positions of RHEED beams can generally be predicted by kinematical scattering theory, quantitative analysis of RHEED patterns relies on dynamical calculations. In this chapter, we will first illustrate the quantum mechanical approach for electron diffraction. Then we will outline a few commonly used dynamical theories accompanied by some calculated results.

Based on the first-principles approach, we will consider the fundamental equation that governs the scattering of high-energy electrons in crystals. Before we show the mathematical description, it is important to consider the nature of the events that we are studying. The average distance between successive electrons that strike the crystal in a transmission electron microscope is about 0.2 mm (for 100 keV electrons) if the electron flux is on the order of 1012 s−1 This distance is much larger than the thickness (typically less than 0.5 μm) of the specimen, thus the interaction between any successive incident electrons is extremely weak. Therefore, the interaction between the incident beam and the crystal can be treated one electron at a time. In other words, electron diffraction theory is basically a single-electron scattering theory.

Strictly speaking, scattering of high-energy electrons obeys the Dirac equation. The Dirac equation contains not only the relativistic effects but also electron spin.

Type
Chapter
Information
Publisher: Cambridge University Press
Print publication year: 1996

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Save book to Kindle

To save this book to your Kindle, first ensure [email protected] is added to your Approved Personal Document E-mail List under your Personal Document Settings on the Manage Your Content and Devices page of your Amazon account. Then enter the ‘name’ part of your Kindle email address below. Find out more about saving to your Kindle.

Note you can select to save to either the @free.kindle.com or @kindle.com variations. ‘@free.kindle.com’ emails are free but can only be saved to your device when it is connected to wi-fi. ‘@kindle.com’ emails can be delivered even when you are not connected to wi-fi, but note that service fees apply.

Find out more about the Kindle Personal Document Service.

  • Dynamical theories of RHEED
  • Zhong Lin Wang, Georgia Institute of Technology
  • Book: Reflection Electron Microscopy and Spectroscopy for Surface Analysis
  • Online publication: 18 January 2010
  • Chapter DOI: https://doi.org/10.1017/CBO9780511525254.005
Available formats
×

Save book to Dropbox

To save content items to your account, please confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your account. Find out more about saving content to Dropbox.

  • Dynamical theories of RHEED
  • Zhong Lin Wang, Georgia Institute of Technology
  • Book: Reflection Electron Microscopy and Spectroscopy for Surface Analysis
  • Online publication: 18 January 2010
  • Chapter DOI: https://doi.org/10.1017/CBO9780511525254.005
Available formats
×

Save book to Google Drive

To save content items to your account, please confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your account. Find out more about saving content to Google Drive.

  • Dynamical theories of RHEED
  • Zhong Lin Wang, Georgia Institute of Technology
  • Book: Reflection Electron Microscopy and Spectroscopy for Surface Analysis
  • Online publication: 18 January 2010
  • Chapter DOI: https://doi.org/10.1017/CBO9780511525254.005
Available formats
×