Shallow Donor Formation In Hydrogen-Implanted Silicon

Published online by Cambridge University Press:  15 February 2011

Yutaka Tokuda
Affiliation:
Department of Electronics, Aichi Institute of Technology, Yakusa, Toyota 470–03, Japan, [email protected]
Hiroyuki Iwata
Affiliation:
Research Institute for Industrial Technology, Aichi Institute of Technology, Yakusa, Toyota 470–03, Japan
Akira Ito
Affiliation:
Department of Electronics and Information Engineering, Suzuka College of Technology, shiroko, Suzuka 510–02, Japan
Get access

Abstract

Formation of shallow donors has been studied in 100-keV hydrogen-implanted n-type silicon with a dose of 1×1015 cm−2. Annealing experiments are made in the temperature range 100 to 800°C. Gold Schottky contacts are fabricated on these samples to obtain carrier concentration profiles. The hydrogen profiles are measured by secondary ion mass spectroscopy. In the annealing temperature range 350 to 450°C, an increase of the carrier concentration is observed near the surface region with almost flat depth profiles. The well- known hydrogen-related donors (1st shallow donors) disappear around 400°C, while shallow donors (2nd shallow donors)observed here decrease above 500 °C. Hydrogen profiles show almost no change in the 2nd donor formation temperatures, although hydrogen starts to outdiffuse at 250°C. This indicates that the 2nd shallow donors are related to hydrogen atoms and to implantation-induced damage. The implantation-induced defects trap diffusing hydrogen atoms, which leads to the formation of the 2nd shallow donors.

Type
Research Article
Copyright
Copyright © Materials Research Society 1997

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Pankove, J. I. and Johnson, N. M., Hydrogen in Semiconductors (Academic, New York, 1991).Google Scholar
2. Pearton, S. J.. Corbett, J.W. and Stavola, M., Hydrogen in Crystalline Semiconductors (Springer, Berlin, 1992).Google Scholar
3. Zohsta, Y., Ohmura, Y. and Kanazawa, M., Japan J. Appl. Phys. 10, 532 (1971).Google Scholar
4. Gorelkinskii, Y. V. and Nevinnyi, N. N., Nucl. Instrum. Methods. 209/210, 677 (1983).Google Scholar
5. Ntsoenzok, E., Desgardin, P., Saillard, M., Vernois, J. and Barbot, J. F., J.Appl. Phys. 79, 8274 (1996).Google Scholar
6. Tokuda, Y., Hasebe, Y., Ito, A., Iwata, H., Usami, A., Terashima, A., Ohshima, H. and Hattori, T., to be published in Semicond. Sci. Technol.Google Scholar
7. Chuengang, L., Yaoxin, L., Chsengtai, S. and Janhua, Y., in Proceedings of the 4th International Conference on Neutron Transmutation Doping in Semiconductors, edited by Larrabe, R. D. (Plenum, New York, 1983), p. 193.Google Scholar
8. Zhengyuan, W. and Lanying, L., in Proceedings of the 4th lnternational Conference on Neutron Transmutation Doping in Semiconductors, edited by Larrabe, R.D. (Plenum, New York, 1983), p.311.Google Scholar
9. Maekevich, V. P., Suezawa, M., Sumino, K. and Murin, L. I., J. Appl. Phys. 76. 7347 (1994).Google Scholar
10. Hatakeyama, H., Suezawa, M., Markevich, V. P. and Sumino, K., in Proceedings of the Materials Science Forum Vols, edited by Suezawa, M. and Katayania-Yoshida, H. (Trans Tech Publications, Switzerland, 1995), p. 939.Google Scholar
11. Hartung, J. and Weber, J., Phys. Rev. B 48, 14161 (1993).Google Scholar
12. Kimerling, L. C., J. Appl. Phys. 45, 1839 (1974).Google Scholar
13. Palmetshofer, L. and Reisinger, J., J. Appl. Phys. 72, 2167 (1992).Google Scholar