Hostname: page-component-586b7cd67f-vdxz6 Total loading time: 0 Render date: 2024-11-24T16:55:33.492Z Has data issue: false hasContentIssue false

Microstructure-Property Relationships in Wear Resistant Alumina/SiC 'nanocomposites' the Importance of Plastic Deformation in Ceramics

Published online by Cambridge University Press:  26 February 2011

Richard Ian Todd
Affiliation:
[email protected], University of Oxford, Department of Materials, Parks Road, Oxford, OX1 3PH, United Kingdom, +44 1865 273718/271718, +44 1865 273783
Apichart Limpichaipanit
Affiliation:
[email protected], University of Oxford, Department of Materials, Parks Road, Oxford, OX1 3PH, United Kingdom
Jose Ortiz Merino
Affiliation:
[email protected], GE-CIAT, Queretaro, CP.76030, Mexico
Get access

Abstract

Alumina/SiC “nanocomposites" consist of a dispersion of submicron SiC particles in an alumina matrix. The resistance to severe wear of the nanocomposites and the surface finish produced by a given grinding treatment are strikingly superior to those of pure alumina with the same grain size. We have explored the reasons for this by correlating a wide range of variations in the basic microstructure with the wear behaviour observed, including both the wear rate, and quantitative surface fractography of the worn surfaces. These improved properties of the nanocomposites are shown to be a consequence of a reduction in surface grain pullout by brittle fracture. In “dilute” nanocomposites (<10% SiC), this is due largely to a reduction in size of the individual pullouts. With 10% SiC nanoparticles, however, there is also evidence that the SiC directly suppresses the nucleation of cracking by plastic deformation of the surface. The origin of these effects will be discussed.

Type
Research Article
Copyright
Copyright © Materials Research Society 2007

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Niihara, K., J. Ceram. Soc. Jpn, 99 (1991) 974982 10.2109/jcersj.99.974Google Scholar