Hostname: page-component-586b7cd67f-vdxz6 Total loading time: 0 Render date: 2024-12-01T10:51:39.886Z Has data issue: false hasContentIssue false

Measurement of initial dissolution rate of P0798 simulated HLW glass by using micro-reactor flow-through test method

Published online by Cambridge University Press:  15 February 2011

H. Makigaki
Affiliation:
Department of Applied Quantum Physics & Nuclear Engineering, Kyushu University, Japan
Y. Inagaki
Affiliation:
Department of Applied Quantum Physics & Nuclear Engineering, Kyushu University, Japan
K. Idemitsu
Affiliation:
Department of Applied Quantum Physics & Nuclear Engineering, Kyushu University, Japan
T. Arima
Affiliation:
Department of Applied Quantum Physics & Nuclear Engineering, Kyushu University, Japan
S. Mitsui
Affiliation:
Geological Isolation Research and Development Directorate, Japan Atomic Energy Agency, Japan
T. Banba
Affiliation:
Nuclear Safety Research Center, Japan Atomic Energy Agency, Japan
K. Noshita
Affiliation:
Energy & Environmental Systems R&D Laboratory, Hitachi, Ltd, Japan
Get access

Abstract

We applied a new type of flow-through test method using micro-reactor consisting of a simple test apparatus with compact size to measurement of the dissolution rate of a Japanese type of simulated waste glass (P0798 glass). In this test method, a solution flows through a micro-channel (20 mm length, 2 mm width, 0.16 mm depth) in contact with a face of coupon shaped glass specimen, and the output solution is retrieved at certain intervals to be analyzed for determination of the glass dissolution rate. By using this test method the initial dissolution rate of glass matrix or forward dissolution rate was measured as a function of pH (3 to 11) and temperature (25°C to 90°C). The present test results indicated that the initial dissolution rate has ‘V-shaped’ pH dependence, and the effect of pH on the dissolution rate decreases with increase in temperature similar to the results measured by using the Single-pass flow-through (SPFT) method. The present test results also indicated that the dissolution of B is controlled by diffusion process and that of Si is controlled by surface reaction process.

Type
Research Article
Copyright
Copyright © Materials Research Society 2009

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1 Strachan, D.M., Bourcier, W.L., McGrail, B.P., Radioactive Waste Management and Environmental Restration, 19(1994)129.Google Scholar
2 Inagaki, Y., Furuya, H. et al. , J.Nucl.Mater. 208(1994)27.Google Scholar
3 Parkhurst, D.L., Water-Resouces Investigations Report 95-4227, US Geological Suvey, 1995 Google Scholar
4 Inagaki, Y., Mitsui, S. et al. “Measurement of HLW glass dissolution/alteration kinetics by using micro-reactor flow-through test method”, these proceedings.Google Scholar
5 Grambow, B., in Scientific Basis for Nuclear Waste Management VIII, edited by Jantzen, C.M., Stone, J.A. and Ewing, R.C. (Mat.Res.Soc.Symp.Proc., Vol.44), p.15(1985).Google Scholar
6 Knauss, K.G., Boucier, W.L. et al. , in Scientific Basis for Nuclear Waste Management XIII, edited by Obversby, V.M. and Brown, P.W. (Mat.Res.Soc.Symp.Proc., Vol.176), p.371(1990).Google Scholar
7 Advocat, T., Crovisier, J.L. et al. , in Scientific Basis for Nuclear Waste Management XIV, edited by Abrajano, T. Jr., Johnson, L.H. (Mat.Res.Soc.Symp.Proc., Vol.212), p.57(1991).Google Scholar
8 Grambow, B., Muller, R., J.Nucl.Mater. 298 (2001)112.Google Scholar
9 Ferrand, K., Abdelouas, A. et al. , J.Nucl.Mater. 355 (2006)54.Google Scholar
10 McGrail, B.P., Ebert, W.L. et al. , J.Nucl.Mater. 249 (1997)175.Google Scholar