Hostname: page-component-586b7cd67f-g8jcs Total loading time: 0 Render date: 2024-11-27T22:17:01.807Z Has data issue: false hasContentIssue false

Material Properties, Thermal Stabilities and Electrical Characteristics of Ge MOS Devices, Depending on Oxidation States of Ge Oxide: Monoxide [GeO(II)] and Dioxide [GeO2(IV)]

Published online by Cambridge University Press:  31 January 2011

Yoshiki Kamata
Affiliation:
[email protected], MIRAI-Toshiba, Kawasaki, Japan
Akira Takashima
Affiliation:
[email protected], Toshiba corporation, Corporate R&D center, Kawasaki, Japan
Tsutomu Tezuka
Affiliation:
[email protected], MIRAI-Toshiba, Kawasaki, Japan
Get access

Abstract

Ge monoxide [GeO(II)] and dioxide [GeO2(IV)], which are selectively formed on Ge substrate by controlling pH and redox potential in pretreatment solution, are confirmed by XPS. ΔEC in GeO(II)/Ge and GeO2(IV)/Ge are almost the same, whereas ΔEV in GeO(II)/Ge is smaller than that in GeO2(IV)/Ge, resulting in smaller Eg of GeO(II). GeO(g) desorption is suppressed in LaAlO3/Ge gate stack, whereas GeO(g) desorbs through LaAlO3 layer when there is an intentional interfacial GeO(II) layer, leading to a large increase in Jg. GeO(g) desorption temperature in Ge oxide/Ge gate stacks decreases with the increase in the ratio of GeO(II) in Ge oxide and is independent of the oxidation techniques. Since GeO(g) desorption is accompanied by H2O(g) desorption, a new model to explain the GeO(g) desorption phenomena is proposed, in which Ge(OH)2 decomposes into GeO(g) and H2O(g). Highly effective etching methods of Ge oxide, using HCl solution and HCl vapor at higher temperature than boiling point of Ge (hydro-)chloride are demonstrated.

Type
Research Article
Copyright
Copyright © Materials Research Society 2009

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1 Kamata, Y., Materials Today 11, 3038 (2008).Google Scholar
2 Kamata, Y., Tutorial H, Materials Research Society Spring Meeting 2008 Google Scholar
3 Pourbaix, M., “Atlas of Electrochemical Equilibria in Aqueous Solutions”. (Pergamon Press, London, 1966).Google Scholar
4 Greenwood, N. N. and Earnshaw, A., “Chemistry of the Elements”, 2nd ed. (Pergamon, Oxford, 1997).Google Scholar
5 Prabhakaran, K., Maeda, F., Watanabe, Y. and Ogino, T., Appl. Phys. Lett. 76, 2244 (2000).Google Scholar
6 Matsubara, H., Sasada, T., Takenaka, M. and Takagi, S., Appl. Phys. Lett. 93, 32104 (2008).Google Scholar
7 Nishimura, T., Lee, C. H., Kita, K., Nagashio, K. and Toriumi, A., Extended Abstract of 2008 International Workshop on Dielectric Thin Film for Future ULSI Devices (IWDTF), 81 (2008).Google Scholar
8 Kamata, Y., Ino, T., Koyama, M. and Nishiyama, A., Appl. Phys. Lett. 92, 63512 (2008).Google Scholar
9 Sakuraba, M., Matsuura, T. and Murota, J., Mater. Res. Soc. Symp. Proc. 535, 281 (1999).Google Scholar
10 Onsia, B., Conard, T., Gendt, S. D., Heyns, M., Hoflijk, I., Mertens, P., Meuris, M., Raskin, G., Sioncke, S., Teerlinck, I., Theuwis, A., Steenbergen, J. V. and Vinckier, C., Diffus. Defect Data B, Solid State Phenom. 103-104, 27 (2005).Google Scholar
11 Sun, S., Sun, Y., Liu, Z., Lee, D.-I., Peterson, S. and Pianetta, P., Appl. Phys. Lett. 88, 21903 (2006).Google Scholar
12 Chui, C. O., Ramanathan, S., Triplett, B. B., McIntyre, P. C. and Saraswat, K. C., IEEE Electron Device Lett. 23, 473 (2002).Google Scholar