Hostname: page-component-586b7cd67f-g8jcs Total loading time: 0 Render date: 2024-11-28T01:50:32.896Z Has data issue: false hasContentIssue false

High Efficiency P3HT/PCBM Solar Cell

Published online by Cambridge University Press:  01 February 2011

Kanzan Inoue
Affiliation:
NanoTech Institute, The University of Texas at Dallas, 2601 N. Floyd Rd. Richardson, TX 75083, USA. Department of Physics, The University of Texas at Dallas, 2601 N. Floyd Rd. Richardson, TX 75083, USA.
Ross Ulbricht
Affiliation:
NanoTech Institute, The University of Texas at Dallas, 2601 N. Floyd Rd. Richardson, TX 75083, USA.
Pallavi C. Madakasira
Affiliation:
NanoTech Institute, The University of Texas at Dallas, 2601 N. Floyd Rd. Richardson, TX 75083, USA. Department of Physics, The University of Texas at Dallas, 2601 N. Floyd Rd. Richardson, TX 75083, USA.
Miaoxin Zhou
Affiliation:
Department of Chemistry, The University of Texas at Dallas, 2601 N. Floyd Rd. Richardson, TX 75083, USA.
Sergey B. Lee
Affiliation:
NanoTech Institute, The University of Texas at Dallas, 2601 N. Floyd Rd. Richardson, TX 75083, USA.
John Ferraris
Affiliation:
NanoTech Institute, The University of Texas at Dallas, 2601 N. Floyd Rd. Richardson, TX 75083, USA. Department of Physics, The University of Texas at Dallas, 2601 N. Floyd Rd. Richardson, TX 75083, USA.
Anvar A. Zakhidov
Affiliation:
NanoTech Institute, The University of Texas at Dallas, 2601 N. Floyd Rd. Richardson, TX 75083, USA. Department of Physics, The University of Texas at Dallas, 2601 N. Floyd Rd. Richardson, TX 75083, USA.
Get access

Abstract

We report a nearly twofold increase of short circuit current: from Isc ∼ 10 mA/cm2 to Isc = 16–20 mA/cm2 in P3HT/PCBM solar cells (SC) employing freshly prepared regio-regular poly(3-hexylthiophene) (RR-P3HT) without special purification. The power conversion efficiency is enhanced to η≥ 4% as compared to our best η=3.8% in SC with commercial polymer despite the decreased filling factor (FF= 0.42, as compared to best FF = 0.59). We used our earlier found [1] procedures with optimal post heat treatment temperatures and time for our polymer SC. We also discovered a strong correlation between the device preparation procedures and performance. The optimal phase separation of PCBM and RR-P3HT into a bi-continuous network structure occurs after quite long solution stirring times (enhanced homogenization) and surprisingly very short annealing time at optimal temperature. We also found that the optimal concentration of PCBM in a RR-P3HT matrix is rather low, only c∼35 wt%, contrary to high c∼80 wt% in PPV based SC.

Type
Research Article
Copyright
Copyright © Materials Research Society 2005

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. a) Inoue, K., Ulbricht, R., Madakasira, P.C., Sampson, W.M., Lee, S., Zakhidov, A.A., Proc. of ICSM 2003, Synth. Met. (2004) (in press);Google Scholar
b) Inoue, K., Ulbricht, R., Madakasira, P. C., Sampson, W.M., Lee, S., Gutierrez, J., Ferraris, J.P., Zakhidov, A.A., Proc. of SPIE – Org. Photovoltaics V, Volume 5520, 256 (2004).Google Scholar
2. Padinger, F., Rittberger, R.S., Sariciftci, N.S., Adv. Funct. Mater. 13, 85 (2003).Google Scholar
3. Yang, X., van Duren, J.J.K., Janssen, R.A.J., Michels, M.A.J., Loos, J., Macromolecules 37, 2151 (2004).Google Scholar
4. van Duren, J.J.K., Loos, J., Morrissey, F., Leewis, C.M., Kivits, K.P.H., van IJzendoorn, L.J., Rispens, M.T., Hummelen, J.C., Janssen, R.A.J., Adv. Funct. Mater. 12, 665 (2002).Google Scholar
5. Camaioni, N., Ridolfi, G., Casalbore-Miceli, G., Possamai, G., Maggini, M. Adv. Mater. 14, 1735–38 (2002).Google Scholar
6. Pham, C.V.; Mark, H.B. Jr; Zimmer, H. Synth. Commun. 16, 689696 (1986).Google Scholar
7. Loewe, R.S.; Khersonsky, S.K.; Mc Cullough, R.D. Adv. Mater. 3, 250 (1999).Google Scholar
8. Loewe, R.S.; Ewbank, P.C.; Liu, J.; Zhai, L.; Mc Cullough, R.D. Macromolecules 34, 43244333 (2001).Google Scholar