Fabrication of GaN with Buried Tungsten (W) Structures Using Epitaxial Lateral Overgrowth (ELO) via LP-MOVPE

Published online by Cambridge University Press:  03 September 2012

Hideto Miyake
Affiliation:
Dept. of Electrical and Electronic Engineering, Mie University, 1515 Kamihama, Tsu, Mie, 514-8507, Japan
Motoo Yamaguchi
Affiliation:
Dept. of Electrical and Electronic Engineering, Mie University, 1515 Kamihama, Tsu, Mie, 514-8507, Japan
Masahiro Haino
Affiliation:
Dept. of Electrical and Electronic Engineering, Mie University, 1515 Kamihama, Tsu, Mie, 514-8507, Japan
Atsushi Motogaito
Affiliation:
Dept. of Electrical and Electronic Engineering, Mie University, 1515 Kamihama, Tsu, Mie, 514-8507, Japan
Kazumasa Hiramatsu
Affiliation:
Dept. of Electrical and Electronic Engineering, Mie University, 1515 Kamihama, Tsu, Mie, 514-8507, Japan
Shingo Nambu
Affiliation:
Dept. of Electronic Engineering, Nagoya University, Furo, Chikusa, Nagoya, 464-8603
Yasutoshi Kawaguchi
Affiliation:
Dept. of Electronic Engineering, Nagoya University, Furo, Chikusa, Nagoya, 464-8603
Nobuhiko Sawaki
Affiliation:
Dept. of Electronic Engineering, Nagoya University, Furo, Chikusa, Nagoya, 464-8603
Yasushi Iyechika
Affiliation:
Tsukuba Research Laboratory, Sumitomo Chemical Co., Ltd, 6 Kitahara, Tsukuba, 300-3294, Japan
Takayoshi Maeda
Affiliation:
Tsukuba Research Laboratory, Sumitomo Chemical Co., Ltd, 6 Kitahara, Tsukuba, 300-3294, Japan
Isamu Akasaki
Affiliation:
Dept. of Electrical and Electronic Engineering, Meijo University, 1-501 Shiogamaguchi, Tempaku, Nogoya 468-8502, Japan
Get access

Abstract

A buried tungsten (W) mask structure with GaN is successfully obtained by epitaxial lateral overgrowth (ELO) technique via low-pressure metalorganic vapor phase epitaxy (LP-MOVPE). The selectivity of GaN growth on the window region vs. the mask region is good. An underlying GaN with a striped W metal mask is easily decomposed above 500 °C by the W catalytic effect, by which radical hydrogen is reacted with GaN. It is difficult to bury the W mask because severe damage occurs in the GaN epilayer under the mask. It is found that an underlying AlGaN/GaN layer with a narrow W stripe mask width (mask/window = 2/2 νm) leads the ELO GaN layer to be free from damage, resulting in an excellent W-buried structure.

Type
Research Article
Copyright
Copyright © Materials Research Society 1999

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1 Nakamura, S., Senoh, M., Nagahama, S., Iwasa, N., Yamada, T., Matsushita, T., Kiyoku, H., Sugimoto, Y., Kozaki, T., Umemoto, H., Sano, M. and Chocho, K., Jpn. J. Appl. Lett. 36 (1997) L1568.Google Scholar
2 Vetury, R., Marchand, H., Parish, G., Fini, P. T., Ibbetson, J. P., Keller, S., Speck, J. S., DenBaars, S. P. and Mishra, U. K., Inst. Phys. Conf. Ser. No. 162: Chapter5 (1999) 177.Google Scholar
3 Ujiie, Y. and Nishinaga, T., Jpn. J. Appl. Phys. 28 (1989) L327.Google Scholar
4 Usui, A., Sunakawa, H., Sakai, A. and Yamaguchi, A., Jpn. J. Appl. Phys. 36 (1997) L899.Google Scholar
5 Sone, H., Nambu, S., Kawaguchi, Y., Yamaguchi, M., Miyake, H., Hiramatsu, K., Iyechika, Y., Maeda, T. and Sawaki, N., Jpn. J. Appl. Phys. 38 (1999) L356.Google Scholar
6 Asai, H., Adachi, S., Ando, S. and Oe, K., J. Appl. Phys. 55 (1984) 3868 Google Scholar
7 Kawaguchi, Y., Nambu, S., Sone, H., Yamaguchi, M., Miyake, H., Hiramatsu, K., and Sawaki, N., Jpn. J. Appl. Phys. 37 (1998) L845.Google Scholar
8 Miyake, H., Motogaito, A. and Hiramatsu, K., Jpn. J. Appl. Phys. 38 (1999) L1000.Google Scholar
9 Hiramatsu, K., Matsushima, H., Hanai, H. and Sawaki, N.: Mat. Res. Soc. Symp. Proc. 482 (1998) 991.Google Scholar