Hostname: page-component-586b7cd67f-t7czq Total loading time: 0 Render date: 2024-11-24T11:02:56.978Z Has data issue: false hasContentIssue false

Electrical Characteristics of the Pt/SBT/TiO2/Si MFIS Structures with Thickness Variation of the SBT Film

Published online by Cambridge University Press:  21 March 2011

Ji-Woong Kim
Affiliation:
Department of Metallurgical Engineering and Materials Science, Hong Ik University, Seoul 121-791, Korea
Kwang-Yong Lee
Affiliation:
Department of Metallurgical Engineering and Materials Science, Hong Ik University, Seoul 121-791, Korea
Jae-Hoon Choi
Affiliation:
Department of Metallurgical Engineering and Materials Science, Hong Ik University, Seoul 121-791, Korea
Tae-Sung Oh
Affiliation:
Department of Metallurgical Engineering and Materials Science, Hong Ik University, Seoul 121-791, Korea
Get access

Abstract

Pt/Sr0.85Bi2.4Ta2O9/TiO2/Si structures were prepared with variation of the Sr0.85Bi2.4Ta2O9 (SBT) film thickness for MFIS-FET applications. After depositing TiO2 film of 10 nm thickness by reactive sputtering on Si(100) substrate as a buffer layer, SBT thin film of 210-400 nm thickness was prepared onto it by metal organic decomposition process. Regardless of the SBT film thickness, the Pt/SBT/TiO2/Si structures exhibited clockwise directional hysteresis, indicating well-defined ferroelectric switching behavior of the SBT films. While the memory window of the Pt/SBT/TiO2/Si MFIS structures increased with increasing the SBT film thickness, the maximum capacitance of the Pt/SBT/TiO2/Si MFIS structures decreased with increasing the SBT film thickness. The Pt/SBT(400 nm)/TiO2(10 nm)/Si structure exhibited a memory window of 1.3 V at ±5 V.

Type
Research Article
Copyright
Copyright © Materials Research Society 2001

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

[1] Scott, J. F. and Araujo, C. A. Paz de, Science 246, 1400 (1989).Google Scholar
[2] Araujo, C. A., Cuchiaro, J. D., McMillan, L. D., Scott, M. C. and Scott, J. F., Nature 374, 627(1995)Google Scholar
[3] Vascankumar, C. V. R., Pascual, R. and Sayer, M., J. Appl. Phys. 71, 864 (1992)Google Scholar
[4] Nagashima, K., Hirai, T., Koike, H., Fujisaki, Y. and Tarui, Y., Jpn. J. Appl. Phys. 35, 1680 (1996).Google Scholar
[5] Fujimori, Y., Izumi, N., Nakamura, T. and Kamisawa, A., IEICE TRANS. ELECTRON. E81, NO.4 (1998).Google Scholar
[6] Kanashima, T. and Okuyama, M., Jpn. J. Appl. Phys. 38, 2044 (1999).Google Scholar
[7] Senzaki, J., Kurihara, K., Nomura, N. and Mitsunaga, O., Jpn. J. Appl. Phys. 37, 5150 (1998).Google Scholar
[8] Tahan, D. M., Safari, A. and Klein, L. C., J. Am. Ceram. Soc. 79, 1594 (1996)Google Scholar
[9] Desu, S. B., Peng, C. H., Kamnerdiana, I. and Schnele, P. J., Mat. Res. Soc. Symp. Proc. 200, 319 (1990)Google Scholar
[10] Zhu, J., Zhang, X., Zhu, Y. and Desu, S. B., J. Appl. Phys. 83, 1610 (1998)Google Scholar