Hostname: page-component-586b7cd67f-r5fsc Total loading time: 0 Render date: 2024-11-25T02:55:54.825Z Has data issue: false hasContentIssue false

Electrical and Microstructural Changes of β-PVDF under Different Processing Conditions by Scanning Force Microscopy

Published online by Cambridge University Press:  01 February 2011

J. Serrado Nunes
Affiliation:
[email protected], University of Minho, Physics, Campus de Gualtar, 4710-057 Braga, Portugal, Braga, 4710-057, Portugal
V. Sencadas
Affiliation:
[email protected], Universidade do Minho, Dept. Física, Campus de Gualtar, Braga, 4710-057, Portugal
A. Wu
Affiliation:
[email protected], Universidade de Aveiro, Dept. Eng. Cerâmica e do Vidro, Campus Universitário de Santiago, Aveiro, 3810-193, Portugal
A. L. Kholkin
Affiliation:
[email protected], Universidade de Aveiro, Dept. Eng. Cerâmica e do Vidro, Campus Universitário de Santiago, Aveiro, 3810-193, Portugal
P. M. Vilarinho
Affiliation:
[email protected], Universidade de Aveiro, Dept. Eng. Cerâmica e do Vidro, Campus Universitário de Santiago, Aveiro, 3810-193, Portugal
S. Lanceros-Méndez
Affiliation:
[email protected], Universidade do Minho, Dept. Física, Campus de Gualtar, Braga, 4710-057, Portugal
Get access

Abstract

Poly vinylidene fluoride (PVDF) has been widely investigated due to its important pyro- and piezoelectric properties. These properties have found various applications, especially as sensor and actuators. The existence and optimization of these properties is intimately related with the fraction of the polymer in the crystalline phase, its structure, microstructure and orientation. All of these in turn heavily depend on the processing conditions. PVDF is a semi-crystalline polymer which shows polymorphism and is commonly crystallized in non-polar crystalline α-phase. The piezo- and pyroelectric properties mainly depend on the β-phase, so that increasing β-phase content has always been of great concern in this field.

β-phase can be obtained by mechanical stretching of α-phase films at a given temperature or directly from solution. Conversion of α into β-phase takes place at stretching temperatures below 100 °C, at a stretch ratio of about 3–5. Nevertheless the achieved amount of β-phase in the crystalline fraction of the material is never 100%. In the films obtained from solution, 100% beta phase films can be achieved in either a porous or non-porous form. The degree of crystallinity is also larger for the samples obtained from solution.

This work is mainly devoted to the study of the variations in the topological morphology and piezoelectric domain response of PVDF prepared by the aforementioned methods by scanning force microscopy in a piezo-response mode.

Type
Research Article
Copyright
Copyright © Materials Research Society 2007

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Lovinger, A. J. In: Developments in Crystalline Polymers; Basset, D.C., Ed. Applied Science Publications: London, 1981.Google Scholar
2. Salimi, A.; Yousefi, A. A., Polym. Testing, 22, 699, 2003.Google Scholar
3. Sencadas, V.; Moreira, V. M.; Lanceros-Mendez, S.; Pouzada, A. S.; Gregorio, Jr., R., Mat. Sci. Forum, 514–16, 872, 2006.Google Scholar
4. Gregorio, Jr., R.; Ueno, E. M., J. Mat. Sci., 34, 4489, 1999.Google Scholar
5. Lanceros-Mendez, S.; Mano, J.F.; Costa, A M.; Schimidt, V.H., J. Macromol. Sci. Physics, B40(3&4), 517, 2001.Google Scholar
6. Gregorio, Jr.,R.; Cestari, M., J. Polym. Sci. Part B: Polym. Phys., 32, 859, 1994.Google Scholar
7. Sencadas, V., Gregorio, Jr., R., Lanceros-Mendez, S., J.Non-Crystalline Solids, 352, 2226, 2006.Google Scholar
8. Lanceros-Mendez, S.; Sencadas, V.; Gregorio, Jr., R., Portuguese patent n0 103318, 2005.Google Scholar