(1-x)(Bi0.8Gd0.2)FeO3-xPbTiO3 (BGF-PT) solid solutions ceramics of x=0.55,0.50,0.4975, 0.49 and 0.45 were prepared by the mixed oxide method. Gd3+ of 20 at% was introduced into the Bi3+ site to improve the dielectric and piezoelectric properties of BFPT without causing the significant reduction of Curie temperature (Tc). X-ray diffraction analysis shows a transformation from the tetragonal (T) to rhombohedral (R) phase with the increase of BGF content. The morphotropic phase boundary was determined by measuring the dielectric and piezoelectric properties of BGF-PT within a wide composition range. BGF-PT for x=0.4975 shows the coexistence of T and R phases with the dielectric constant and loss of about 895 and 0.031 respectively at the frequency of 102 Hz.