Deposition of Highly (100) Oriented PZT Film Using Lanthanum Nitrate/Nickel Acetate Buffer Layer
Published online by Cambridge University Press: 26 February 2011
Abstract
Highly (100) oriented Pb(Zr,Ti)O3 [PZT] films were fabricated using lanthanum nitrate/nickel acetate double layers as a buffer layer, regardless of the other deposition conditions, such as the pyrolysis temperature, pyrolysis time, annealing temperature, and heating rate. The buffer layer was also acted as a very effective barrier against Pb-Si interdiffusion, thus allowing for the direct deposition of PZT films on Si, SiO2/Si, and glass substrates. The strong orientation was attributed to the formation of a crystalline intermediate phase between the PZT and lanthanum nitrate during annealing. The lanthanum nitrate/nickel acetate double layers became a lanthanum nickel oxide (LaNiO3), which shows good electrical conductivity, after an annealing process at 650°C. The nature and the role of lanthanum nitrate buffer as a layer for the growth of highly (100) oriented PZT films have been studied. The dielectric, ferroelectric, piezoelectric and electrooptic properties of the highly (100) oriented PZT films with a lanthanum nitrate/nickel acetate buffer layer were measured and compared with the values measured from the (111) and (100) oriented PZT films deposited without buffer layer.
Keywords
- Type
- Research Article
- Information
- MRS Online Proceedings Library (OPL) , Volume 902: Symposium T – Ferroelectric Thin Films XIII , 2005 , 0902-T03-23
- Copyright
- Copyright © Materials Research Society 2006