Hostname: page-component-586b7cd67f-gb8f7 Total loading time: 0 Render date: 2024-11-28T07:54:01.283Z Has data issue: false hasContentIssue false

Control of Residual Stresses in As-Grown Polysilicon by Multi-Layer Deposition: The “Multipoly” Process

Published online by Cambridge University Press:  10 February 2011

Hie Yang
Affiliation:
Department of Materials Science and Engineering, Case Western Reserve University, Cleveland, Ohio
H. Kahn
Affiliation:
Department of Materials Science and Engineering, Case Western Reserve University, Cleveland, Ohio
A.Q. He
Affiliation:
Department of Materials Science and Engineering, Case Western Reserve University, Cleveland, Ohio
S.M. Phillips
Affiliation:
Department of Electrical Engineering and Computer Science, Case Western Reserve University, Cleveland, Ohio
A.H. Heuer
Affiliation:
Department of Materials Science and Engineering, Case Western Reserve University, Cleveland, Ohio
Get access

Abstract

LPCVD polysilicon thin films deposited between ∼550 and ∼600 °C have an equiaxed microstructure (resulting from crystallization of an initially amorphous deposit) and contain ∼200 MPa residual tensile stresses after deposition, whereas polysilicon films deposited above ∼600 °C have a columnar microstructure and contain ∼300 MPa residual compressive stresses after deposition. Both types of films also contain stress gradients.

We have grown films containing multiple layers of polysilicon ("MultiPoly") by cycling the growth temperature between 570 and 615 °C. The multilayer films thus formed are comprised of alternating tensile and compressive layers, and by control of the thickness of the individual layers, the overall stress of the polysilicon can display any value between that of the tensile layer and that of the compressive layer. We have focussed on producing films with zero overall residual stress, as measured by wafer curvature, and have characterized the microstructures by transmission electron microscopy (TEM) and X-ray diffraction (XRD).

Because of the stress gradients present in both layers, devices made from films with zero overall residual stress may show distortions after release. We have measured the stress gradients in each type of layer and can design films with zero overall stress and zero overall stress gradients. It is also possible to design films with any level of overall (tensile or compressive) stress but with controlled displacements upon release.

Type
Research Article
Copyright
Copyright © Materials Research Society 2000

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

[1] Joubert, P., Loisel, B., Chouan, Y., and Haji, L., “The effect of low pressure on the structure of LPCVD polycrystalline silicon films,” J. Electrochem. Soc., vol. 134, no. 10, pp. 25412544, Oct. 1987 Google Scholar
[2] Kakinuma, H., “Comprehensive interpretation of the preferred orientation of vapor-phase grown polycrystalline silicon films,” J. Vac.Sci. Technol.A., Vol. 13, No.5, pp 23102317, Sep/Oct 1995 Google Scholar
[3] Huang, J., Krulevitch, P., Johnson, G.C., Howe, R.T., and Wenk, H.R., “Investigation of texture and stress in undoped polysilicon films,” MRS Symposium Proceedings, Vol. 182, pp. 201206, 1990 10.1557/PROC-182-201Google Scholar
[4] Krulevitch, P.A., Howe, R.T., Johnson, G.C., and Huang, J., “Stress in undoped LPCVD polycrystalline silicon,” Proc. IEEE Conf. on Solid-state Sensors and Actuators, Transducers 91, pp. 949952, 1991.Google Scholar
[5] Guckel, H., Sniegowski, J.J., Christenson, T.R., and Raissi, F., “The application of fine-grained, tensile polysilicon to mechanically resonant transducers,” Sensors and Actuators A, A21-A23, 346351, 1990 Google Scholar
[6] Guckel, H., Burns, D.W., Visser, C.C.G., Tilmans, H.A.C., and Deroo, D., “Fine-grained polysilicon films with built-in tensile strain,", IEEE Trans. on Electron Devices, Vol. 35, no. 6, pp.800801, 1988.10.1109/16.2534Google Scholar
[7] Yu, C.-L., Flinn, P.A., Lee, S.-H., and Bravman, J.C., “Stress and microstructural evolution of LPCVD polysilicon thin films during high temperature annealing,” MRS Symposium Proceedings, Vol. 441, pp. 403408.Google Scholar
[8] Kahn, H., Stemmer, S., Nandakumar, K., Heuer, A.H., Mullen, R.L., Ballarini, R., and Huff, M.A., “Mechanical properties of thick, surface micromachined polysilicon films,” Proc. IEEE Micro Electro Mech. Syst. Workshop, MEMS 96, San Diego, CA, pp.343348, 1996 Google Scholar