Article contents
Aluminum and boron diffusion in 4H-SiC
Published online by Cambridge University Press: 11 February 2011
Abstract
A brief survey is given of some recent result of boron diffusion in low doped n-type (intrinsic) and p-type 4H-SiC. Aluminum diffusion and solubility limit in 4H-SiC are also discussed. Ion implantation of boron has been performed in epitaxial material to form a diffusion source but also epitaxial 4H-SiC structures, with heavily boron or aluminum doped layers prepared by vapor phase epitaxy have been studied. Heat treatments have been made at temperatures ranging from 1100 to 2050°C for 5 minutes up to 64 h. Secondary ion mass spectrometry has been utilized for analysis. For boron diffusion in acceptor doped 4H-SiC, 4×1019 Al atoms/cm3, an activation energy of 5.3 eV has been determined and a strong dependence on Al content for the diffusion coefficient is revealed. Transient enhanced diffusion of ion-implanted boron in intrinsic 4H-SiC samples is discussed. Solubility limits of ∼1×1020 Al/cm3 (1700°C) and <1×1020 B/cm3 (1900°C) have been deduced.
- Type
- Research Article
- Information
- Copyright
- Copyright © Materials Research Society 2003
References
REFERENCES
- 6
- Cited by