Hostname: page-component-586b7cd67f-vdxz6 Total loading time: 0 Render date: 2024-11-28T08:05:33.207Z Has data issue: false hasContentIssue false

Study on Resistance Increase Trends and Recovery Characteristics of YBCO Thin-film Wire According to Insulation Layer

Published online by Cambridge University Press:  21 April 2011

Ho Ik Du
Affiliation:
Advance Graduate Education Center of Jeonbuk for Electronics and Information Technology-BK21, Chonbuk National University, 664-14, 1 Ga Duckjin-Dong, Jeonju-Shi, S. Korea
Byoung Sung Han
Affiliation:
Electrical Engineering, Chonbuk National University, 664-14, 1 Ga Duckjin-Dong, Jeonju-Shi, S. Korea
Yong Jin Kim
Affiliation:
Electrical Engineering, Chonbuk National University, 664-14, 1 Ga Duckjin-Dong, Jeonju-Shi, S. Korea
Dong Hyeok Lee
Affiliation:
Electrical Engineering, Chonbuk National University, 664-14, 1 Ga Duckjin-Dong, Jeonju-Shi, S. Korea
Sang Seob Song
Affiliation:
Electronics Science Engineering, Chonbuk National University, 664-14, 1 Ga Duckjin-Dong, Jeonju-Shi, S. Korea
Get access

Abstract

To apply the superconducting wire to power machines, it is necessary to conduct research on the characteristics of wire phase changes in connection with insulating layers. In this study, according to the presence or absence of insulating layers in the wire, and to the thickness of such layers, the wire's resistance increase trends and the characteristics of its recovery from quenching were examined by current-applied cycle at the temperatures of 90 K, 180 K and 250 K. Towards this end, YBCO thin-film wires that have the same critical temperatures and that have copper and stainless-steel stabilizing layers were prepared. One level and three and five levels of superior-performance polyimide pressure-sensitive adhesive tape was attached to the wires at a very low temperature. The eight prepared test samples were wound around the linear frames, then the wire's voltage and current created owing to the phase change characteristics were measured at each prescribed temperature, using the four-point probe method. Further, near the examination temperatures of 90 K, 180 K and 250 K the wire's resistance and recovery characteristics were examined by cycle.

Type
Research Article
Copyright
Copyright © Materials Research Society 2010

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Ishiyama, A., Ueda, H., Ando, T., Naka, H., Bamba, S. and Shiohara, Y., IEEE Trans. Appl. Supercond. 17, 2430 (2007).Google Scholar
2. Du, H. I., Yim, S. W., Choi, B. J., Choi, B. H., Doo, S. G., Han, B. S., Han, Y. H. and Sung, T. H., Physica C 468, 1706 (2008).Google Scholar
3. Watanabe, T., Shiohara, Y. and Izumi, T., IEEE Trans. Appl. Supercond. 13, 2445 (2003).Google Scholar
4. Amemiya, N., Murasawa, S., Banno, N. and Miyamoto, K., Physica C 310, 16 (1998).Google Scholar
5. Du, H. I., Yim, M. J., Doo, S. G., Kim, Y. J., Han, B. S., Trans. KEEE 10, 62 (2009).Google Scholar