Hostname: page-component-586b7cd67f-vdxz6 Total loading time: 0 Render date: 2024-11-28T08:06:37.313Z Has data issue: false hasContentIssue false

Study of the Macrosegregation of Silicon in Steels for Electrical Applications

Published online by Cambridge University Press:  14 February 2012

V. A. Aranda Villada
Affiliation:
Departamento de Ingeniería Metalúrgica, Facultad de Química, Edif. D, UNAM, Ciudad Universitaria, Coyoacán, México D. F. CP 04510;
J. A. García Hinojosa
Affiliation:
Departamento de Ingeniería Metalúrgica, Facultad de Química, Edif. D, UNAM, Ciudad Universitaria, Coyoacán, México D. F. CP 04510;
H. Cruz Mejía
Affiliation:
Departamento de Ingeniería Metalúrgica, Facultad de Química, Edif. D, UNAM, Ciudad Universitaria, Coyoacán, México D. F. CP 04510;
A. A. Balandra Aranzueta
Affiliation:
Departamento de Ingeniería Metalúrgica, Facultad de Química, Edif. D, UNAM, Ciudad Universitaria, Coyoacán, México D. F. CP 04510;
M. G. González F
Affiliation:
Departamento de Ingeniería Metalúrgica, Facultad de Química, Edif. D, UNAM, Ciudad Universitaria, Coyoacán, México D. F. CP 04510;
Y. Houbaert
Affiliation:
Department of Metallurgy and Materials Science, Ghent University, B-9052 Zwijnaarde, Belgium
Get access

Abstract

Macrosegregation is harmful to the material properties (strength, corrosion resistance, etc.) and it must be avoided or eliminated from castings. In this work, macrosegregation behavior is evaluated in terms of silicon concentration in cast ingots of steels with 0.5, 1.5 and 3 wt% Si. The dimensions of the castings are 25x30x12.5 cm. The Si segregation profiles are evaluated in three zones: upper, middle and bottom of each ingot. The characterization is carried out by energy dispersive spectrometry in at least 10 positions of each zone of the ingot. Silicon analysis is evaluated from the surface to the centre of each ingot. The experimental results are compared with predictions using an Experimental Segregation Index (ESI) and the Scheil Segregation Index (SSI). The experimental results show a strong deviation from the profiles predicted by the Scheil model. The evaluation of the degree of segregation by "ESI" indicates little variation of silicon from the surface to the center of the ingot showing a uniform distribution across the ingot analyzed.

Type
Articles
Copyright
Copyright © Materials Research Society 2012

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Ferreira, I. L., Spinellia, J. E. and Garcia, A., J. Alloys Compd., 475, 396 (2009).Google Scholar
2. Prabhakar, B., M. S Thesis, University of British Columbia, 1973 Google Scholar
3. Liu, Y. L, and Kang, S. B, Mater. Sci. Technol., 13, 331 (1997)Google Scholar
4. Kato, H., Cahoon, J.R., Metal. Mater Trans. A, 16, 579 (1985)Google Scholar
5. Flemings, M.C. and Nereo, G.E., Trans TMS-AIME, 239, 1449 (1967)Google Scholar
6. Yang, W., Chen, W., Minn, K., Mannan, S. and de Barbadillo, J., Metal. Mater Trans. A, 32, 397 (2001)Google Scholar
7. Kurz, W., and Trivedi, R., Metal and Mater Trans A, 27, 625, (1996)Google Scholar
8. Gu, J.P and Beckermann, C. Metal Mater Trans A, 30, 1357, (1999)Google Scholar
9. González, M. G., Noguez, A. M. E., Principios de Microscopía Electrónica de Barrido y Microanálisis por Rayos X,(UNAM, Facultad de Química, 2006), 120134.Google Scholar
10. Battle, T.P. and Pehlke, R.D., Metal and Mater Trans B, 21, 357 (1990)Google Scholar