Hostname: page-component-586b7cd67f-dlnhk Total loading time: 0 Render date: 2024-11-24T08:26:42.056Z Has data issue: false hasContentIssue false

Dispersions of Surface Modified Calcium Hydroxide Nanoparticles with Enhanced Kinetic Stability: Properties and Applications to Desalination and Consolidation of the Yungang Grottoes

Published online by Cambridge University Press:  22 August 2014

Ya Xiao
Affiliation:
State Key Laboratory for Powder Metallurgy, Central South University, Changsha, China, 410083 Cultural Relics and Archaeology Institute of Hunan Province, Changsha, China, 410083
Feng Gao
Affiliation:
State Key Laboratory for Powder Metallurgy, Central South University, Changsha, China, 410083 Chinese Academy of Cultural Heritage, Beijing 100029, China
Yun Fang
Affiliation:
China University of Geosciences (Wuhan), Wuhan, 430074, China
Youdan Tan
Affiliation:
School of Chemistry and Chemical Engineering, Central South University, Changsha 410083, China
Kaiyu Liu*
Affiliation:
School of Chemistry and Chemical Engineering, Central South University, Changsha 410083, China
Shaojun Liu*
Affiliation:
State Key Laboratory for Powder Metallurgy, Central South University, Changsha, China, 410083 School of Chemistry and Chemical Engineering, Central South University, Changsha 410083, China
*
*Email: [email protected] (S.J. Liu)
Get access

Abstract

Calcium hydroxide (Ca(OH)2) is one of the most interesting materials used to consolidate stone sculptures, monuments, mortars or wall paintings. In this study, we reported on the synthesis and characterization of surface modified Ca(OH)2 nanoparticles as a dispersion with enhanced kinetic stability and the applications for the conservation of sandstone monuments. Uniform hexagonal Ca(OH)2 nanoparticles (∼35nm) were obtained by mixing NaOH and NaCl aqueous solutions at 100∼175oC using homogeneous-phase reactions. It was further demonstrated that 3-(Methacryloyloxypropane oxygen) trimethoxysilane surfactant agent can significantly reduce agglomeration and simultaneously improve specific surface area of as-synthesized Ca(OH)2 nanoparticles. Brunauer-Emmett-Teller (BET) measurement showed that specific surface area of modified Ca(OH)2 nanoparticles reaches up to ∼48.78m2/g, about 2.5 and 3.4 times higher than that of unmodified and commercial ones, respectively. The kinetic stability of Ca(OH)2 despersion can be further enhanced and its viscosity can be decreased by optimizing the ratio of ethanol and n-propanol. Especially, a technique, which combined the Ferroni-Dini method and dispersion of Ca(OH)2 nanoparticles with enhanced kinetic stability, was proposed to effectively desalinate and consolidate the decayed stone, as evidenced by significant decreases of the porosity and concentration of detrimental Cl- and SO42- ions in the severely decayed sandstone samples from the Yungang grottoes.

Type
Articles
Copyright
Copyright © Materials Research Society 2014 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

Gómez-Ortíz, N., De la Rosa-García, S., González-Gómez, W., Soria-Castro, M., Quintana, P., Oskam, G., and Ortega-Morales, B., ACS Appl. Mater. Inter. 5, 1556 (2013).10.1021/am302783hCrossRefGoogle Scholar
Tiano, P., Cantisani, E., Sutherland, I., Paget, J., J. Cult. Herit. 7, 49 (2006).10.1016/j.culher.2005.10.003CrossRefGoogle Scholar
Daniele, V., Taglieri, G., Quaresima, R., J. Cult. Herit. 11, 294 (2008).10.1016/j.culher.2007.10.007CrossRefGoogle Scholar
Ambrosi, M., Dei, L., Giorgi, R., Neto, C., Baglioni, P., Langmuir. 17, 4251 (2001).10.1021/la010269bCrossRefGoogle Scholar
López-Arce, P., Gómez, L., Pinho, L., Fernández-Valle, M., Álvarez de Buergo, M., Fort, R., Mater. Charact. 61, 168 (2010).10.1016/j.matchar.2009.11.007CrossRefGoogle Scholar
Yasue, T., Tsuchida, Y. and Arai, Y., Gypsum. Lime. 189, 17 (1984).Google Scholar
Nanni, A., Dei, L., Langmuir. 19, 933 (2003).10.1021/la026428oCrossRefGoogle Scholar
Daniele, V., Taglieri, G., J. Cult. Herit. 13, 40 (2012).10.1016/j.culher.2011.05.007CrossRefGoogle Scholar
Salvadori, B., Dei, L., Langmuir. 17, 2371 (2001).10.1021/la0015967CrossRefGoogle Scholar
Perez-Maqueda, L. A., Wang, L. and Matijevic, E., Langmuir. 14, 4397 (1998).10.1021/la980149cCrossRefGoogle Scholar
Ambrosi, M., Dei, L., Giorgi, R, Neto, C., Baglioni, P., Prog. Colloid Polym. Sci. 118, 68 (2001).10.1007/3-540-45725-9_15CrossRefGoogle Scholar
Baglioni, P., Giorgi, R., Soft. Matter. 2, 293 (2006).10.1039/b516442gCrossRefGoogle Scholar
Huang, J., J. Yanbei Normal Univ. 19(5), 57 (2003).Google Scholar
Yuan, J., Feng, X., World Antiquity. 5, 74 (2004).Google Scholar
Li, Z., World. Antiquity. 5, 3 (2004).Google Scholar
Espinosa-Marzal, R., Scherer, G., Accounts. Chem. Res. 43, 695 (2010).10.1021/ar9002224CrossRefGoogle Scholar
Scherer, G, Flatt, R, Wheeler, G, MRS Bull. 26, 44 (2001).10.1557/mrs2001.18CrossRefGoogle Scholar
Tian, S, Liu, S, Gao, F, Fan, M, Ren, J, Mater. Res. Soc. Symp. Proc. 1319, Boston, MA, 2010, DOI: 10.1557/opl.2011.Google Scholar
Liu, S., Sun, M., Gao, F., Xiao, Y., Liu, K., J. Central. South. Univ: Sci.. & Tech. 44(1), 46 (2011).Google Scholar
Yura, K., Fredrikson, K., Matijevic, E., Colloids Surf. A. 50, 281 (1990).10.1016/0166-6622(90)80270-ECrossRefGoogle Scholar
Rees, G., Evans-Gowing, R., Hammond, S., Robinson, B., Langmuir. 15, 1999 (1993).Google Scholar