Hostname: page-component-586b7cd67f-t8hqh Total loading time: 0 Render date: 2024-11-28T16:01:50.462Z Has data issue: false hasContentIssue false

Crystal Structure and Thermoelectric Properties of Al-containing Re Silicides

Published online by Cambridge University Press:  26 February 2011

Eiji Terada
Affiliation:
Department of Materials Science and Engineering, Kyoto University, Sakyo-ku, Kyoto 606–8501, Japan
Min-Wook Oh
Affiliation:
Department of Materials Science and Engineering, KAIST, Yuseong-gu, Daejon 305–701, Republic of Korea
Dang-Moon Wee
Affiliation:
Department of Materials Science and Engineering, KAIST, Yuseong-gu, Daejon 305–701, Republic of Korea
Haruyuki Inui
Affiliation:
Department of Materials Science and Engineering, Kyoto University, Sakyo-ku, Kyoto 606–8501, Japan
Get access

Abstract

The microstructure, defect structure and thermoelectric properties of Al-containing ReSi1.75 based silicides have been investigated. All the Al-containing alloys investigated contain four differently oriented domains accompanied by the twinned microstructure, as the binary alloy does. However, thin defect layers containing a kind of shear structure are locally and sporadically formed at some of twin boundaries. In the defect layer, shear occurs by the vector of [100] on either (1 09) or (107) planes. Binary ReSi1.75 exhibits nice thermoelectric properties as exemplified by the high value of dimensionless figure of merit (ZT) of 0.70 at 800 °C when measured along [001], although the ZT value along [100] is just moderately high. Al-containing Re silicides considerably increase the ZT value along [100] so that the maximum value of 0.95 is achieved at 150 °C for the ReSi1.75Al0.02 alloy. The temperature dependence of electrical resistivity changes from of semiconductor for the binary alloy to of metal for the Al-added alloys and the value of electrical resistivity is significantly reduced when compared to the binary counterpart.

Type
Research Article
Copyright
Copyright © Materials Research Society 2005

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Heinrich, A., Griebmann, H., Behr, G., Ivanenko, L., Schumann, J. and Vinzelberg, H., Thin Solid Films 381, 287 (2001).Google Scholar
2. Becker, J.P.. Mahan, J.E. and Long, R.G., J. Vac. Sci. Tech. A, 13, 1133 (1995)Google Scholar
3. Gu, J-J, Kuwabara, K., Tanaka, K., Inui, H., Yamaguchi, M., Yamamoto, A., Ohta, T. and Obara, H. in Defect Properties and Related Phenomena in Intermetallic Alloys, edited by George, E. P., Inui, H., Mills, M. J., and Eggeler, G., (Mater. Res. Soc. Proc. 753, Boston, Massachusetts, 2002) p. 501506.Google Scholar
4. Sakamaki, Y., Kuwabara, K., Jiajun, Gu, Inui, H., Yamaguchi, M., Yamamoto, A. and Obara, H., Materials Science Forum 426–432, 17331738 (2003).Google Scholar
5. Siegrist, T., Hulliger, F. and Travaglini, G., J. Less-Common Met. 92, 119 (1983).Google Scholar
6. Neshpor, V. S. and Samsonov, G. V., Izv. Akad. Nauk S.S.S.R., Neorg. Mater. 1, 655 (1965) [Inorg. Mater. (U.S.S.R.) 1, 599 (1965)].Google Scholar
7. Neshpor, V. S. and Samsonov, G. V., Fiz. Met. Metalloved. 11, (4) 638 (1961) [Sov. Phys.-Phys. Met. Metallogr. 11, (4) 146(1961)].Google Scholar