Abstract

In order to decrease the silica content in 16% Cr ferritic stainless steel, the phases present in deoxidized inclusions were predicted by the FACT model. To decrease the amount of deoxidized inclusions and slag inclusions in the melt, the capacity of alumina absorption was compared using different top slags. In trial tests, the cleanliness of slabs was significantly improved in 16% Cr ferritic stainless steel produced by AOD processes and the number of surface defects of cold coils was also significantly reduced.

Type
Research Article
Copyright
© La Revue de Métallurgie, 2004

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)