Cristobalite transformation in two refractory materials with 45 and 42 % alumina

Published online by Cambridge University Press:  25 October 2002

Get access

Abstract

A natural kaolin material, which contains 45 wt % of alumina and less than 1 wt % of metal oxide impurities, has been submitted to thermal treatments in the temperature range 1 000-1 450 °C. The cristobalite development is studied by X-ray diffraction, using the broadening of line {101}. The apparent grain sizes of cristobalite, measured by the integral width of the line, change as a function of thermal treatment. Nevertheless, the apparent total content of the cristobalite remains constant. In the case of a chamotte material, which contains 42 wt % alumina and 3 to 4 wt % of metal oxide impurities, the apparent cristobalite grain sizes are of order of magnitude of the nanometer and the total apparent content is slightly lower. Finally, the thermal expansion coefficient, α (T), of the first material is higher, during the cristobalite transformation αβ, than that of the chamotte material.

Type
Research Article
Copyright
© La Revue de Métallurgie, 2002

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)