Ti–Si–C–N thin films grown by reactive arc evaporation from Ti3SiC2 cathodes

Published online by Cambridge University Press:  16 March 2011

Anders O. Eriksson*
Affiliation:
Thin Film Physics Division, Department of Physics, Chemistry, and Biology (IFM), Linköping University, SE-581 83 Linköping, Sweden
Jianqiang Zhu
Affiliation:
Nanostructured Materials, Department of Physics, Chemistry, and Biology (IFM), Linköping University, SE-581 83 Linköping, Sweden
Naureen Ghafoor
Affiliation:
Nanostructured Materials, Department of Physics, Chemistry, and Biology (IFM), Linköping University, SE-581 83 Linköping, Sweden
Jens Jensen
Affiliation:
Thin Film Physics Division, Department of Physics, Chemistry, and Biology (IFM), Linköping University, SE-581 83 Linköping, Sweden
Grzegorz Greczynski
Affiliation:
Thin Film Physics Division, Department of Physics, Chemistry, and Biology (IFM), Linköping University, SE-581 83 Linköping, Sweden
Mats P. Johansson
Affiliation:
Nanostructured Materials, Department of Physics, Chemistry, and Biology (IFM), Linköping University, SE-581 83 Linköping, Sweden; andSeco Tools AB, SE-737 82 Fagersta, Sweden
Jacob Sjölen
Affiliation:
Seco Tools AB, SE-737 82 Fagersta, Sweden
Magnus Odén
Affiliation:
Nanostructured Materials, Department of Physics, Chemistry, and Biology (IFM), Linköping University, SE-581 83 Linköping, Sweden
Lars Hultman
Affiliation:
Thin Film Physics Division, Department of Physics, Chemistry, and Biology (IFM), Linköping University, SE-581 83 Linköping, Sweden
Johanna Rosén
Affiliation:
Thin Film Physics Division, Department of Physics, Chemistry, and Biology (IFM), Linköping University, SE-581 83 Linköping, Sweden
*
a)Address all correspondence to this author. e-mail: [email protected]
Get access

Abstract

Ti–Si–C–N thin films were deposited onto WC-Co substrates by industrial scale arc evaporation from Ti3SiC2 compound cathodes in N2 gas. Microstructure and hardness were found to be highly dependent on the wide range of film compositions attained, comprising up to 12 at.% Si and 16 at.% C. Nonreactive deposition yielded films consisting of understoichiometric TiCx, Ti, and silicide phases with high (27 GPa) hardness. At a nitrogen pressure of 0.25–0.5 Pa, below that required for N saturation, superhard, 45–50 GPa, (Ti,Si)(C,N) films with a nanocrystalline feathered structure were formed. Films grown above 2 Pa displayed crystalline phases of more pronounced nitride character, but with C and Si segregated to grain boundaries to form weak grain boundary phases. In abundance of N, the combined presence of Si and C disturbs cubic phase growth severely and compromises the mechanical strength of the films.

Type
Articles
Copyright
Copyright © Materials Research Society 2011

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1.Flink, A., Beckers, M., Sjölen, J., Larsson, T., Braun, S., Karlsson, L., and Hultman, L.: The location and effects of Si in (Ti1– xSi x)Ny thin films. J. Mater. Res. 24, 2483 (2009).CrossRefGoogle Scholar
2.Karlsson, L., Hultman, L., Johansson, M.P., Sundgren, J.E., and Ljungcrantz, H.: Growth, microstructure, and mechanical properties of arc evaporated TiC xN1– x (0 ≤ x ≤ 1) films. Surf. Coat. Techol. 126, 1 (2000).CrossRefGoogle Scholar
3.Abraham, S., Choi, E.Y., Kang, N., and Kim, K.H.: Microstructure and mechanical properties of Ti-Si-C-N films synthesized by plasma-enhanced chemical vapor deposition. Surf. Coat. Techol. 202, 915 (2007).CrossRefGoogle Scholar
4.Kuo, D.-H. and Huang, K.-W.: A new class of Ti-Si-C-N coatings obtained by chemical vapor deposition, Part 1: 1000 °C process. Thin Solid Films 394, 72 (2001).Google Scholar
5.Kuo, D.-H. and Huang, K.-W.: A new class of Ti-Si-C-N coatings obtained by chemical vapor deposition—Part II: Low-temperature process. Thin Solid Films 394, 81 (2001).Google Scholar
6.Kuo, D.-H. and Liao, W.-C.: A new class of Ti-Si-C-N coatings obtained by chemical vapor deposition, Part III: 650–800 °C process. Thin Solid Films 419, 11 (2002).CrossRefGoogle Scholar
7.Guo, Y., Ma, S.L., and Xu, K.W.: Effects of carbon content and annealing temperature on the microstructure and hardness of super hard Ti-Si-C-N nanocomposite coatings prepared by pulsed d.c. PCVD. Surf. Coat. Techol. 201, 5240 (2007).Google Scholar
8.Jedrzejowski, P., Klemberg-Sapieha, J.E., and Martinu, L.: Quaternary hard nanocomposite TiCxNy/SiCN coatings prepared by plasma enhanced chemical vapor deposition. Thin Solid Films 466, 189 (2004).Google Scholar
9.Ma, D.Y., Ma, S.L., Dong, H.S., Xu, K.W., and Bell, T.: Microstructure and tribological behavior of super-hard Ti-Si-C-N nanocomposite coatings deposited by plasma enhanced chemical vapour deposition. Thin Solid Films 496, 438 (2006).Google Scholar
10.Ma, D.Y., Ma, S.L., and Xu, K.W.: Superhard nanocomposite Ti-Si-C-N coatings prepared by pulsed-d.c plasma enhanced CVD. Surf. Coat. Techol. 200, 382 (2005).Google Scholar
11.Shtansky, D.V., Levashov, E.A., Sheveiko, A.N., and Moore, J.J.: The structure and properties of Ti-B-N, Ti-Si-B-N, Ti-Si-C-N, and Ti-Al-C-N coatings deposited by magnetron sputtering using composite targets produced by self-propagating high-temperature synthesis (SHS). J. Mater. Synth. Process. 6, 61 (1998).Google Scholar
12.Shtansky, D.V., Levashov, E.A., Sheveiko, A.N., and Moore, J.J.: Synthesis and characterization of Ti-Si-C-N films. Metall. Mater. Trans. A 30, 2439 (1999).Google Scholar
13.Xu, H., Nie, X., and Wei, R.: Tribological behavior of a TiSiCN coating tested in air and coolant. Surf. Coat. Techol. 201, 4236 (2006).CrossRefGoogle Scholar
14.Wei, R.H., Langa, E., Rincon, C., and Arps, J.H.: Deposition of thick nitrides and carbonitrides for sand erosion protection. Surf. Coat. Techol. 201, 4453 (2006).CrossRefGoogle Scholar
15.Jeon, J.-H., Choi, S.R., Chung, W.S., and Kim, K.H.: Synthesis and characterization of quaternary Ti-Si-C-N coatings prepared by a hybrid deposition technique. Surf. Coat. Techol. 188189, 415 (2004).CrossRefGoogle Scholar
16.Johnson, L.J.S., Rogström, L., Johansson, M.P., Odén, M., and Hultman, L.: Microstructure evolution and age hardening in (Ti, Si)(C, N) thin films deposited by cathodic arc evaporation. Thin Solid Films 519, 1397 (2010).Google Scholar
17.Chang, C.-L. and Hsieh, T.-J.: Effect of C2H2 gas flow rate on synthesis and characteristics of Ti-Si-C-N coating by cathodic arc plasma evaporation. J. Mater. Process. Technol. 209, 5521 (2009).Google Scholar
18.Barsoum, M.W.: A new class of solids: Thermodynamically stable nanolaminates. Prog. Solid State Chem. 28, 201 (2000).Google Scholar
19.Jansson, M.S.: CONTES, Conversion of Time-Energy Spectra—a Program for ERDA Data Analysis, Uppsala University, 2004.Google Scholar
20.Oliver, W.C. and Pharr, G.M.: An improved technique for determining hardness and elastic-modulus using load and displacement sensing indentation experiments. J. Mater. Res. 7, 1564 (1992).CrossRefGoogle Scholar
21.Eriksson, A.O., Zhu, J.Q., Ghafoor, N., Johansson, M.P., Sjölén, J., Jensen, J., Odén, M., Hultman, L., and Rosén, J.: Layer formation by resputtering in Ti-Si-C hard coatings during large scale cathodic arc deposition. Surf. Coat. Technol. DOI: 10.1016/j.surfcoat.2011.02.007 (2011).CrossRefGoogle Scholar
22.Guo, Y., Ma, S.L., Xu, K.W., Bell, T., Li, X.Y., and Dong, H.S.: On the oxidation resistance of superhard Ti-Si-C-N coatings.:J. Mater. Res. 23, 2420 (2008).Google Scholar
23.PDF: TiN 00-038-1420, TiC 00-032-1383, Ti 00-044-1294, TiSi2 00-035-0785, Ti5Si3 00-029-1362, ICDD “Powder Diffraction File” (2008).Google Scholar
24.Sue, J.A.: X-ray elastic constants and residual stress of textured titanium nitride coating. Surf. Coat. Techol. 5455, 154 (1992).Google Scholar
25.Flink, A., Larsson, T., Sjölen, J., Karlsson, L., and Hultman, L.: Influence of Si on the microstructure of arc evaporated (Ti, Si)N thin films; evidence for cubic solid solutions and their thermal stability. Surf. Coat. Techol. 200, 1535 (2005).Google Scholar
26.Marten, T., Isaev, E.I., Alling, B., Hultman, L., and Abrikosov, I.A.: Single-monolayer SiNx embedded in TiN: A first-principles study. Phys. Rev. B 81, 212102 (2010).Google Scholar
27.Hultman, L., Bareño, J., Flink, A., Söderberg, H., Larsson, K., Petrova, V., Odén, M., Greene, J.E., and Petrov, I.: Interface structure in superhard TiN-SiN nanolaminates and nanocomposites: Film growth experiments and ab initio calculations. Phys. Rev. B 75, 155437 (2007).CrossRefGoogle Scholar
28.Snis, A. and Matar, S.F.: Electronic density of states, 1s core-level shifts, and core ionization energies of graphite, diamond, C3N4 phases, and graphitic C11N4. Phys. Rev. B 60, 10855 (1999).Google Scholar
29.Lu, Y.H., Shen, Y.G., Zhou, Z.F., and Li, K.Y.: Phase configuration, nanostructure evolution, and mechanical properties of unbalanced magnetron-sputtered Ti-Cx-Ny thin films. J. Vac. Sci. Technol. A 25, 1539 (2007).CrossRefGoogle Scholar
30.Hellgren, N., Johansson, M.P., Broitman, E., Hultman, L., and Sundgren, J.-E.: Role of nitrogen in the formation of hard and elastic CNx thin films by reactive magnetron sputtering. Phys. Rev. B 59, 5162 (1999).CrossRefGoogle Scholar
31.Neidhardt, J., Hultman, L., and Czigány, Z.: Correlated high resolution transmission electron microscopy and x-ray photoelectron spectroscopy studies of structured CNx (0 < x < 0.25) thin solid films. Carbon 42, 2729 (2004).Google Scholar
32.Anders, A.: A structure zone diagram including plasma-based deposition and ion etching. Thin Solid Films 518, 4087 (2010).Google Scholar
33.Anders, A.: Cathodic Arcs, Chapter 6(Springer, New York, 2008).Google Scholar
34.Rosén, J., Anders, A., Mraz, S., Atiser, A., and Schneider, J.M.: Influence of argon and oxygen on charge-state-resolved ion-energy distributions of filtered aluminum arcs. J. Appl. Phys. 99, 123303 (2006).CrossRefGoogle Scholar
35.Eklund, P.: Novel ceramic Ti-Si-C nanocomposite coatings for electrical contact applications. Surf. Eng. 23, 406 (2007).CrossRefGoogle Scholar