Hostname: page-component-586b7cd67f-gb8f7 Total loading time: 0 Render date: 2024-12-01T02:33:34.919Z Has data issue: false hasContentIssue false

Effect of nickel addition on the exothermic reaction of titanium and boron carbide

Published online by Cambridge University Press:  03 March 2011

Y.F. Yang
Affiliation:
Key Laboratory of Automobile Materials of Ministry of Education and Department of Materials Science and Engineering, Jilin University, Nanling Campus, Changchun 130025, People’s Republic of China
H.Y. Wang
Affiliation:
Key Laboratory of Automobile Materials of Ministry of Education and Department of Materials Science and Engineering, Jilin University, Nanling Campus, Changchun 130025, People’s Republic of China
Y.H. Liang
Affiliation:
Key Laboratory of Automobile Materials of Ministry of Education and Department of Materials Science and Engineering, Jilin University, Nanling Campus, Changchun 130025, People’s Republic of China
R.Y. Zhao
Affiliation:
Key Laboratory of Automobile Materials of Ministry of Education and Department of Materials Science and Engineering, Jilin University, Nanling Campus, Changchun 130025, People’s Republic of China
Q.C. Jiang*
Affiliation:
Key Laboratory of Automobile Materials of Ministry of Education and Department of Materials Science and Engineering, Jilin University, Nanling Campus, Changchun 130025, People’s Republic of China
*
a) Address all correspondence to this author. e-mail: [email protected]
Get access

Abstract

Exothermic reaction path of the Ni–Ti–B4C system in the differential thermal analysis apparatus proceeded in such a way that Ni initially reacted with B4C and Ti to form Ni–B compounds and Ti2Ni with heat release, respectively; subsequently, the formation of Ni–B eutectic liquid between Ni2B and Ni4B3, and the appearance of Ni–Ti eutectic liquid phase between Ti2Ni and Ti were followed, which enabled the diffusion of Ni, B, C, and Ti in solution to form Ni–Ti–B–C liquid more easily and quickly at a low temperature; finally, TiC and TiB2 were precipitated out of the liquid. The addition of Ni provided an easier route for reactant mass transfer and accelerated the occurrence of complete reaction.

Type
Articles
Copyright
Copyright © Materials Research Society 2007

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1Munir, Z.A. and Anselmi-Tamburini, U.: Self–propagating exothermic reactions: The synthesis of high–temperature materials by combustion. Mater. Sci. Reports 3, 277 (1989).CrossRefGoogle Scholar
2Merzhanov, A.G.: Combustion and Plasma Synthesis of High-Temperature Materials, edited by Munir, Z.A. and Holt, J.B. (VCH Publishers, New York, 1990), pp. 153.Google Scholar
3Yi, H.C. and Moore, J.J.: Self–propagating high–temperature (combustion) synthesis (shs) of powder–compacted materials. J. Mater. Sci. 25, 1159 (1990).CrossRefGoogle Scholar
4Wang, L.L., Munir, Z.A., and Maximov, Y.M.: Thermite reactions—their utilization in the synthesis and processing of materials. J. Mater. Sci. 28, 3693 (1993).CrossRefGoogle Scholar
5Telle, R. and Petzow, G.: Strengthening and toughening of boride and carbide hard metal composites. Mater. Sci. Eng., A 105, 97 (1988).CrossRefGoogle Scholar
6Williams, W.S.: Influence of temperature, strain rate, surface condition, and composition on the plasticity of transition–metal carbide crystals. J. Appl. Phys. 35, 1329 (1964).CrossRefGoogle Scholar
7Ramberg, J.R., Wolfe, C.F., and Williams, W.S.: Resistance of titanium diboride to high-temperature plastic yielding. J. Am. Ceram. Soc. 68, 78 (1985).CrossRefGoogle Scholar
8Weimer, A.W.: Carbide Nitride and Boride Materials Synthesis and Processing (Chapman and Hall, London, 1997) pp. 79113.CrossRefGoogle Scholar
9Wen, G., Li, S.B., Zhang, B.S., and Guo, Z.X.: Reaction synthesis of TiB2–TiC composites: With enhanced toughness. Acta Mater. 49, 1463 (2001).CrossRefGoogle Scholar
10Barsoum, M.W. and Houng, B.: Transient plastic phase processing of titanium boron carbon composites. J. Am. Ceram. Soc. 76, 1445 (1993).CrossRefGoogle Scholar
11Zhao, H. and Cheng, Y.B.: Formation of TiB2–TiC composites by reactive sintering. Ceram. Int. 5, 353 (1999).CrossRefGoogle Scholar
12Song, I., Wang, L., Wixom, M., and Thompson, L.T.: Self–propagating high–temperature synthesis and dynamic compaction of titanium diboride/titanium carbide composites. J. Mater. Sci. 35, 2611 (2000).CrossRefGoogle Scholar
13Zhang, X.H., Zhu, C.C., Qu, W., He, X.D., and Kvanin, V.L.: Self– propagating high temperature synthesis of TiC/TiB2 ceramic– matrix composites. Compos. Sci. Technol. 62, 2037 (2002).Google Scholar
14Gotman, I., Travitzky, N.A., and Gutmanas, E.Y.: Dense in situ TiB2/TiN and TiB2/TiC ceramic matrix composites: Reactive synthesis and properties. Mater. Sci. Eng., A 244, 127 (1998).CrossRefGoogle Scholar
15Gotman, I., Koczak, M.J., and Shtessel, E.: Fabrication of Al matrix in situ composites via self–propagating synthesis. Mater. Sci. Eng., A 187, 189 (1994).CrossRefGoogle Scholar
16Tjong, S.C. and Ma, Z.Y.: Microstructural and mechanical characteristics of in situ metal matrix composites. Mater. Sci. Eng., R 29, 49 (2000).CrossRefGoogle Scholar
17Durlu, N.: Titanium based carbide composites for high temperature applications. J. Eur. Ceram. Soc. 19, 2415 (1999).CrossRefGoogle Scholar
18 International Center for Diffraction Data: Powder Diffraction File, Alphabetical Indexes (International Center for Diffraction Data, 2000).Google Scholar
19Liang, Y.J. and Che, Y.C.: Notebook of Thermodynamic Data of Inorganic (East-north University Press, Shen yang, China, 1996) pp. 83382.Google Scholar
20Massalski, T.B., Okamoto, H., Subramanian, P.R., and Kacprzak, L.: Binary Alloy Phase Diagrams (ASM International, Materials Park, OH, 1996).Google Scholar
21Brodkin, D., Kalidindi, S.R., Barsoum, M.W., and Zavaliangos, A.: Microstructural evolution during transient plastic phase processing of titanium carbide-titanium boride composites. J. Am. Ceram. Soc. 79, 1945 (1996).CrossRefGoogle Scholar