Hostname: page-component-586b7cd67f-t8hqh Total loading time: 0 Render date: 2024-11-24T15:30:35.988Z Has data issue: false hasContentIssue false

Improved wettability of Sn-based solder over the Cu60Zr30Ti10 bulk metallic glass surface

Published online by Cambridge University Press:  31 January 2011

S. Maruyama
Affiliation:
Materials and Structures Laboratory (MSL), Tokyo Institute of Technology, Midori-ku, Yokohama 226-8503, Japan
H. Nishikawa
Affiliation:
Joining and Welding Research Institute (JWRI), Osaka University, Ibaraki, Osaka 0047, Japan
M. Fukuhara
Affiliation:
Institute for Materials Research (IMR), Tohoku University, Aoba-ku, Sendai 980-8577, Japan
T. Takemoto
Affiliation:
Joining and Welding Research Institute (JWRI), Osaka University, Ibaraki, Osaka 0047, Japan
A. Inoue
Affiliation:
Institute for Materials Research (IMR), Tohoku University, Aoba-ku, Sendai 980-8577, Japan
Y. Matsumoto*
Affiliation:
Materials and Structures Laboratory (MSL), Tokyo Institute of Technology, Midori-ku, Yokohama 226-8503, Japan
*
a) Address all correspondence to this author. e-mail: [email protected]
Get access

Abstract

The wettability of Pb-free Sn-based solder over the Cu-based Cu60Zr30Ti10 bulk metallic glass surface was investigated. We observed that the as-polished surface was nonwetting for the solder, which was due to the surface oxide layer of ZrOx formed in air. After complete removal of the oxide layer, a thin layer of Ag was deposited on the clean Cu60Zr30Ti10 surface. The Ag-covered Cu60Zr30Ti10 surface showed relatively high resistivity to the reoxidation even in air, and thus the wettability of the Cu60Zr30Ti10 surface for the Sn-based solder was greatly improved.

Type
Articles
Copyright
Copyright © Materials Research Society 2009

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1Inoue, A.: Stabilization of metallic supercooled liquid and bulk amorphous alloys. Acta Mater. 48, 297 (2000)CrossRefGoogle Scholar
2Inoue, A.: Bulk amorphous and nanocrystalline alloys with high functional properties. Mater. Sci. Eng., A 304, 1 (2001)CrossRefGoogle Scholar
3Chen, H.S.: Glassy metals. Rep. Prog. Phys. 43, 353 (1980)CrossRefGoogle Scholar
4Inoue, A., Zhang, W., Zhang, T. and Kurosaka, K.: High-strength Cu-based bulk glassy alloys in Cu–Zr–Ti and Cu–Hf–Ti ternary systems. Acta Mater. 49, 2645 (2001)CrossRefGoogle Scholar
5Carini, J.P., Nagel, S.R., Varga, L.K. and Schmidt, T.: Electronic transport in amorphous Ni1–xPx alloys. Phys. Rev. B 27, 7589 (1983)CrossRefGoogle Scholar
6Gilbert, C.J., Ritchie, R.O. and Johnson, W.L.: Fracture toughness and fatigue-crack propagation in a Zr–Ti–Ni–Cu–Be bulk metallic glass. Appl. Phys. Lett. 71, 476 (1997)CrossRefGoogle Scholar
7Nagel, S.R.: Thermoelectric power and resistivity in a metallic glass. Phys. Rev. Lett. 41, 990 (1978)CrossRefGoogle Scholar
8Nishikawa, H., Piromsarn, K.W., Abe, H., Takemoto, T., Fukuhara, M., Wada, T. and Inoue, A.: Wetting characteristics of Sn–Ag–Cu solder on Pd-based metallic glass. Mater. Sci. Eng., B 148, 124 (2008)CrossRefGoogle Scholar
9Matsumoto, Y., Obata, T., Hiraoka, M. and Katayama, M.: Development of a variable temperature UHV-laser microscope combined with a pulsed laser deposition for in situ studies of ceramics/metallics glass interfaces. Ceram. Trans. 198, 15 (2007)CrossRefGoogle Scholar
10Tam, C.Y. and Shek, C.H.: Oxidation-induced copper segregation in Cu60Zr30Ti10 bulk metallic glass. J. Mater. Res. 21, 851 (2006)CrossRefGoogle Scholar
11Matsumoto, Y., Aibara, Y., Mukai, K., Moriwaki, K., Okawa, Y., Neiuwenhuys, B.E. and Tanaka, K.: STM studies of oxygen-induced reconstruction on a Pt-Rh (100) alloy surface. Surf. Sci. 377, 32 (1997)CrossRefGoogle Scholar