Crossref Citations
This article has been cited by the following publications. This list is generated based on data provided by
Crossref.
Domnich, Vladislav
Gogotsi, Yury
and
Trenary, Michael
2000.
Identification of Pressure-Induced Phase Transformations Using Nanoindentation.
MRS Proceedings,
Vol. 649,
Issue. ,
Bradby, J. E.
Williams, J. S.
Wong-Leung, J.
Swain, M. V.
and
Munroe, P.
2000.
Transmission electron microscopy observation of deformation microstructure under spherical indentation in silicon.
Applied Physics Letters,
Vol. 77,
Issue. 23,
p.
3749.
Bradby, J.E.
Williams, J.S.
Wong-Leung, J.
Swain, M.V.
and
Munroe, P.
2000.
Mechanical Deformation of Crystalline Silicon During Nanoindentation.
MRS Proceedings,
Vol. 649,
Issue. ,
Dub, Sergey N.
Milman, Yuly V.
Lozko, Dina V.
and
Belous, Anton N.
2000.
Mechanism of Al-Cu-Fe Quasicrystal Plastic Deformation Studied by Instrumented Sharp Indentation.
MRS Proceedings,
Vol. 649,
Issue. ,
Domnich, Vladislav
and
Gogotsi, Yury
2001.
Handbook of Surfaces and Interfaces of Materials.
p.
195.
Bradby, J. E.
Williams, J. S.
Wong-Leung, J.
Swain, M. V.
and
Munroe, P.
2001.
Mechanical deformation in silicon by micro-indentation.
Journal of Materials Research,
Vol. 16,
Issue. 5,
p.
1500.
Domnich, V.
and
Gogotsi, Y.
2001.
Frontiers of High Pressure Research II: Application of High Pressure to Low-Dimensional Novel Electronic Materials.
p.
291.
Domnich, Vladislav
and
Gogotsi, Yury
2001.
Advances in Surface Science.
Vol. 38,
Issue. ,
p.
355.
Bradby, J. E.
Williams, J. S.
and
Swain, M. V.
2002.
In-situ electrical characterization of Si during nanoindentation.
MRS Proceedings,
Vol. 750,
Issue. ,
Dub, Sergey
Novikov, Nikolay
and
Milman, Yuly
2002.
The transition from elastic to plastic behaviour in an Al-Cu-Fe quasicrystal studied by cyclic nanoindentation.
Philosophical Magazine A,
Vol. 82,
Issue. 10,
p.
2161.
Bradby, J. E.
Williams, J. S.
Wong-Leung, J.
Swain, M. V.
and
Munroe, P.
2002.
Nanoindentation-induced deformation of Ge.
Applied Physics Letters,
Vol. 80,
Issue. 15,
p.
2651.
Kovalchenko, Andriy
Gogotsi, Yury
Domnich, Vladislav
and
Erdemir, Ali
2002.
Phase Transformations in Silicon Under Dry and Lubricated Sliding.
Tribology Transactions,
Vol. 45,
Issue. 3,
p.
372.
Eyink, K. G.
Grazulis, L.
Reber, J. C.
and
Busbee, J. D.
2002.
Micro-raman study of the damage in nanopatterned GaAs(001).
Journal of Electronic Materials,
Vol. 31,
Issue. 10,
p.
1112.
Algueró, M.
Bushby, A. J.
Reece, M. J.
and
Seifert, A.
2002.
Anelastic deformation of Pb(Zr,Ti)O3 thin films by non-180° ferroelectric domain wall movements during nanoindentation.
Applied Physics Letters,
Vol. 81,
Issue. 3,
p.
421.
Domnich, Vladislav
Gogotsi, Yury
Trenary, Michael
and
Tanaka, Takaho
2002.
Nanoindentation and Raman spectroscopy studies of boron carbide single crystals.
Applied Physics Letters,
Vol. 81,
Issue. 20,
p.
3783.
Colomban, Philippe
and
Havel, Mickael
2002.
Raman imaging of stress‐induced phase transformation in transparent ZnSe ceramic and sapphire single crystals.
Journal of Raman Spectroscopy,
Vol. 33,
Issue. 10,
p.
789.
Li, Z.C
Liu, L
Wu, X
He, L.L
and
Xu, Y.B
2002.
Indentation induced amorphization in gallium arsenide.
Materials Science and Engineering: A,
Vol. 337,
Issue. 1-2,
p.
21.
Juliano, Tom
Gogotsi, Yury
and
Domnich, Vladislav
2003.
Effect of indentation unloading conditions on phase transformation induced events in silicon.
Journal of Materials Research,
Vol. 18,
Issue. 5,
p.
1192.
Grillo, S E
Ducarroir, M
Nadal, M
Tourni , E
and
Faurie, J-P
2003.
Nanoindentation of Si, GaP, GaAs and ZnSe single crystals.
Journal of Physics D: Applied Physics,
Vol. 36,
Issue. 1,
p.
L5.
Ge, Daibin
Domnich, Vladislav
and
Gogotsi, Yury
2003.
High-resolution transmission electron microscopy study of metastable silicon phases produced by nanoindentation.
Journal of Applied Physics,
Vol. 93,
Issue. 5,
p.
2418.