Published online by Cambridge University Press: 06 March 2019
X-ray fractography is a new method utilizing the X-ray diffraction technique to observe the fracture surface for the analysis of the micromechanisms and mechanics of fracture. The line broadening of X-ray diffraction profiles and the residual stress are two of the important X-ray parameters. Among them, the X-ray residual stress has been confirmed to be particularly useful for the fracture surfaces of high strength steels, and applied to the fracture surface of fracture toughness specimens and the fatigue fracture surface.