Low Voltage Sen for Unique Surface Analysis of Prosthetic Devices

Published online by Cambridge University Press:  26 February 2011

Eugene P. Goldberg
Affiliation:
Biomedical Engineering Center, Dept. Materials Science - MAE 217, University of Florida, Gainesville, FL 32611
Moshe Yalon
Affiliation:
Biomedical Engineering Center, Dept. Materials Science - MAE 217, University of Florida, Gainesville, FL 32611
William E. Longo
Affiliation:
Materials Analytical Services, 3597 Parkway Lane - Suite 250, Norcross, GA 30092
Get access

Abstract

Surgical manipulation of plastic prostheses using metal instruments is likely to produce surface damage and surface roughness which may compromise biocompatibility of implants due to tissue irritation and increased cellular or bacterial adhesion. There are virtually no data in the literature concerning the clinical occurrence and consequences of manipulative surface damage to implants. We have found that conventional high voltage scanning electron microscopy techniques (HVSEM) obscure surface defects on plastics due in large measure to beam energy “healing” by local melting. This paper reports the use of low voltage SEM (LVSEN) at low beam voltages (<1.5keV) and without the need for conductive carbon or Au/Pd coatings for examination of plastic device surfaces before and after normal surgical manipulation. Results for intraocular lens implants, a major human prosthesis, clearly demonstrate that standard surgical procedures can produce significant implant surface damage which may not be observed by normal SEN analysis. LVSEN has been shown to readily visualize such previously unobserved surface defects in model surgical manipulation experiments. These results have important implications for more reliable polymer surface characterization and for development of improved prosthetic devices, instruments, and implant surgery.

Type
Research Article
Copyright
Copyright © Materials Research Society 1988

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Sawyer, L.C. and Grubb, L.T., Polymer Microscopy, (Chapman and Hall, London, 1987).CrossRefGoogle Scholar
2. Pawley, J., J. Microscopy, 136, 45 (1984).Google Scholar
3. Kotani, H., Kawabe, M. and Namba, S., Jpn. J. Appl. Phys., 18–2, 279 (1979).CrossRefGoogle Scholar
4. Samoto, N., Shimizu, R. and Hashimoto, H., Jpn. J. Appl. Phys., 24–4, 482 (1985).Google Scholar
5. Erasmus, S.J., J. Vac. Sci. Technol., B5–1, 409 (1987).CrossRefGoogle Scholar
6. Price, C.W. and McCarthy, P.L., Scanning, 10, 29 (1988).CrossRefGoogle Scholar
7. Berry, V.K., Scanning, 10, 19 (1988).Google Scholar
8. Ohara, K., Proc. 3rd World Congress Biomtls. (1988); and private communication.Google Scholar