Hostname: page-component-78c5997874-ndw9j Total loading time: 0 Render date: 2024-11-08T04:28:59.887Z Has data issue: false hasContentIssue false

The Critical Condition for the Initiation of Localized Corrosion of Mild Steels in Contact with Bentonite Used For Nuclear Waste Package

Published online by Cambridge University Press:  25 February 2011

Guen Nakayama
Affiliation:
Research Institute, Ishikawajima-Harima Heavy Industries Co., Ltd. Tokyo 135 Japan
Masatsune Akashi
Affiliation:
Research Institute, Ishikawajima-Harima Heavy Industries Co., Ltd. Tokyo 135 Japan
Get access

Abstract

It has been established that the mild steels which undergo the general corrosion in the acidic to neutral environments, attain the passivity status in alkaline environments, thereby becoming liable to the localized corrosion, such as pitting corrosion and crevice corrosion. Now, for the case of using bentonite as a buffer to stand between the hostrock and the geological disposal packages of high level nuclear waste, localized corrosion behaviors of mild steel as a candidate for such a package has been studied quantitatively for environments where the the otherwise neutral ground water would be turned slightly alkaline with pH = 9.5 - 10.0.

In view of the lack of quantitative data on the passivity-to-localized corrosion of mild steel in natural water environments of weak alkalinity, the present authors have previously determined an empirical E-pH diagram for mild steel with a 20 °C, 1 m mol/L [HC03-], 10 ppm [CI -] solution simulating the natural water environment concerned; it has been shown that the general corrosion-to-passivity transition condition was determined to be pHd =9.4, and the mild steel was shown to be liable to localized corrosion over a large portion of the passivity domain. The present paper discusses behaviors, mechanisms, and critical conditions for initiation of localized corrosion in mild steel placed in bentonitesuspending natural water environment, in terms of the critical potentials for pitting (Vc), and crevice corrosion (ER,CREV). Bentonite was addid to the solution in varying amounts to give bentonite-to-solution ratios up to 0.1, while the pHvalue was adjusted appropriately with sodium carbonate, always keeping the bentonite particles in suspension.

It is demonstrated that bentonite particles suspended in water will deposit upon the steel on receipt of Fe2 + ions, thereby promoting pitting corrosion by preventing repassivation and promoting crevice corrosion by acting as an effective crevice, once the environment conditions become favorable for localized corrosion.

We conclude therefore that disposal package made of mild steel and placed in an underground water environment with bentonite as buffer will be liable to localized corrosion.

Type
Research Article
Copyright
Copyright © Materials Research Society 1992

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

[1] Akashi, M., Fukuda, T., and Yoneyama, H.: “A Corrosion Assessment of Mild Steel Used for Nuclear Waste Package,” Scientific Basis for Nuclear Waste Management XIII, Mat. Res. Soc. Proc. 176, Ed. Oversby, V. M. and Brown, P. W., p. 525 (1990).Google Scholar
[2] Ishikawa, H., Amemiya, K., Yusa, Y., and Sasaki, N.: “Comparison of Fundamental Properties of Japanese Bentonite as Buffer Material for Waste Disposal,” presented to 9th Intern. Clay Conf., Strasbourg, France (1989).Google Scholar
[3] Marsh, G. P., Bland, I. D., Desport, J. A., Naish, C., Westcott, C., and Taylor, K. J.: Europe. Appl. Res. Rep. -Nucl. Sci. Technol., 5 [2], 223 (1983).Google Scholar
[4] Nakayama, G. and Akashi, M.: “The Critical Condition of Localized Corrosion of Mild Steel for Nuclear Waste Package,” Mat. Res. Soc. Symp. proc. 212, p.279 (1991)CrossRefGoogle Scholar
[5] Japan Clay Society, ed.: Clay Handbook, Tokyo: Gihodo (1974) [in Japanese].Google Scholar
[6] Leckin, H. P. and Uhlig, H. H.; J. Electrochem. Soc., 113, 1262 (1966).Google Scholar
[7] Tsujikawa, S. and Hisamatsu, Y.: boshoku Gijutsu, 29, 37 (1980) [in Japanese]Google Scholar
[8] Tsujikawa, S.: “Repassivation Potential as Crevice Corrosion Characteristic for Austenite and Ferritic Stainless Steels,” Proc. 3rd Soviet-Japanese Seminar on Corrosion and Protection, Ed. Kolotyrikin, Ya. M., NAUKA Publishers, p. 119 (1984).Google Scholar
[9] JIS G 0577: “Method of Pitting Potential Measurement for Stainless Steels,” (1981).Google Scholar