Sliding wear performance of thermally sprayed Ni-Cr based alloy deposited on SAE 1045 steel

Published online by Cambridge University Press:  18 October 2019

Edwuin Carrasquero*
Affiliation:
Research Group in Characterization, Processing and Protection of Materials (GICPPM), Universidad Estatal de Milagro (UNEMI), Ecuador
Arnoud Tricoteaux
Affiliation:
UPHF, Département de l’Ingénierie de la Chimie et des Matériaux, Valencienne, France
Jorge Fajardo
Affiliation:
Research Group in New Materials and Processes of Transformation (GiMaT), Universidad Politécnica Salesiana, Calle Vieja 12-30 y Elia Liut, Cuenca, Ecuador
Luis López
Affiliation:
Research Group in New Materials and Processes of Transformation (GiMaT), Universidad Politécnica Salesiana, Calle Vieja 12-30 y Elia Liut, Cuenca, Ecuador
*
*corresponding autor : [email protected]
Get access

Abstract

The present work has been carried out in order to investigate the sliding wear performance of a Ni-Cr based alloy, containing boron, carbon, silicon and iron, deposited onto a SAE 1045 steel substrate. The coatings were thermally sprayed by means of a High Velocity Oxy-Fuel system and post heat-treated for one hour at 760°C in an argon atmosphere. The relative sliding performance was evaluated under unlubricated dry conditions at different applied normal loads and sliding velocities, in order to analyze the influence of these parameters on the wear response. Test results are discussed and interpreted on the basis of both microstructural evaluations and mechanical properties measurements. The surface morphology and topography of the wear scars have been studied through of a Scanning Electron Microscopy (SEM) and Energy Dispersive X-ray Spectroscopy (EDS) techniques. The results have shown an improved wear resistance of the coated steel samples as compared to the uncoated ones.

Type
Articles
Copyright
Copyright © Materials Research Society 2019 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

Serres, N., Hlawka, F., Costil, S., Langlade, C., Machi, F., and Cornet, A., Surface and Coatings Technology 204, 197 (2009).CrossRefGoogle Scholar
Serres, N., Hlawka, F., Costil, S., Langlade, C., and Machi, F., Surface and Coatings Technology 205, 1039 (2010).CrossRefGoogle Scholar
Dong, S., Song, B., Liao, H., and Coddet, C., Surface and Coatings Technology 268, 36 (2015).CrossRefGoogle Scholar
Liu, S., Zheng, X., and Geng, G., Materials & Design 31, 913 (2010).CrossRefGoogle Scholar
Sidhu, T.S., Prakash, S., and Agrawal, R.D., Thin Solid Films 515, 95 (2006).CrossRefGoogle Scholar
Rodrı́guez, J., Martı́n, A., Fernández, R., and Fernández, J.E., Wear 255, 950 (2003).CrossRefGoogle Scholar
Shrestha, S., Hodgkiess, T., and Neville, A., J Therm Spray Tech 10, 656 (2001).CrossRefGoogle Scholar
Planche, M.P., Liao, H., Normand, B., and Coddet, C., Surface and Coatings Technology 200, 2465 (2005).CrossRefGoogle Scholar
Miguel, J.M., Guilemany, J.M., and Vizcaino, S., Tribology International 36, 181 (2003).CrossRefGoogle Scholar
Harsha, S., Dwivedi, D.K., and Agarwal, A., Int J Adv Manuf Technol 38, 93 (2007).CrossRefGoogle Scholar
Houdková, S., Smazalová, E., Vostřák, M., and Schubert, J., Surface and Coatings Technology 253, 14 (2014).CrossRefGoogle Scholar
Bergant, Z. and Grum, J., J Therm Spray Tech 18, 380 (2009).CrossRefGoogle Scholar
Lee, C.H. and Min, K.O., Surface and Coatings Technology 132, 49 (2000).CrossRefGoogle Scholar
Ahmed, R., Yu, H., Edwards, L., and Santisteban, J.R., World Congress on Engineering 2007 (Volume 1) 1181 (2007).Google Scholar
Chicot, D., Araujo, P., Horny, N., Tricoteaux, A., and Lesage, J., Surface and Coatings Technology 200, 174 (2005).CrossRefGoogle Scholar
Chicot, D., Marot, G., Araujo, P., Horny, N., Tricoteaux, A., Staia, M., and Lesage, J., Surface Engineering 22, 390 (2006).CrossRefGoogle Scholar
Asl, Sh.K., Sohi, M.H., Hokamoto, K., and Uemura, M., Wear 260, 1203 (2006).CrossRefGoogle Scholar
Bergant, Z., Trdan, U., and Grum, J., Corrosion Science 88, 372 (2014).CrossRefGoogle Scholar
Gil, L.E., Angulo, N., Minchala, J.M., Romero, B.R., and Carrasquero, E.J., Revista Latinoamericana de Metalurgia y Materiales; Artículos Aceptados (ASAP) (2019).Google Scholar
Lesage, J., Staia, M.H., Chicot, D., Godoy, C., and De Miranda, P.E.V., Thin Solid Films 377–378, 681 (2000).CrossRefGoogle Scholar
Marshall, D.B., Noma, T., and Evans, A.G., Journal of the American Ceramic Society 65, c175 (1982).CrossRefGoogle Scholar
ASTM International, (2010).Google Scholar
Bhat, D.G., Materials and Manufacturing Processes 8, 103 (1993).CrossRefGoogle Scholar
Määttä, A., Kanerva, U., and Vuoristo, P., J Therm Spray Tech 20, 366 (2010).CrossRefGoogle Scholar
Guilemany, J.M., Miguel, J.M., Vizcaı́no, S., Lorenzana, C., Delgado, J., and Sánchez, J., Surface and Coatings Technology 157, 207 (2002).CrossRefGoogle Scholar