Hostname: page-component-cd9895bd7-hc48f Total loading time: 0 Render date: 2024-12-27T07:45:33.178Z Has data issue: false hasContentIssue false

Varying Phases of Alumina Nanowires Templated by Vertically Aligned Carbon Nanotubes Grown via Atomic Layer Deposition

Published online by Cambridge University Press:  27 August 2014

Lester Lampert
Affiliation:
Department of Physics and Department of Mechanical & Materials Engineering, Portland State University, Portland, OR, USA
Sean Smith
Affiliation:
School of Electrical Engineering & Computer Science, Oregon State University, Corvallis, OR, USA
Brittany Timonen
Affiliation:
Department of Physics and Department of Mechanical & Materials Engineering, Portland State University, Portland, OR, USA
John F. Conley Jr.
Affiliation:
School of Electrical Engineering & Computer Science, Oregon State University, Corvallis, OR, USA
Jun Jiao
Affiliation:
Department of Physics and Department of Mechanical & Materials Engineering, Portland State University, Portland, OR, USA

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Abstract
Copyright
Copyright © Microscopy Society of America 2014 

References

[1] Fang, X. S., et al, Journal of Physics: Cond. Matter 16 (2004), p. 4157.Google Scholar
[2] Gu, Z., et al, Nanoscale 1 (2009), p. 347.Google Scholar
[3] Pang, Y. T., et al, J Solid State Electrochem 7 (2003), p. 344.Google Scholar
[4] The authors acknowledge support from the Maseeh College of Engineering at Portland State University.Google Scholar