Hostname: page-component-586b7cd67f-t7fkt Total loading time: 0 Render date: 2024-11-24T21:30:25.236Z Has data issue: false hasContentIssue false

TEM Study of Precipitation Sequences in Haynes 282 Ni Superalloy

Published online by Cambridge University Press:  01 August 2018

A. Alexandratou
Affiliation:
Lab. of Physical Metallurgy, School of Mining and Metallurgical Engineering, National Technical University of Athens, Athens, Greece
S. Deligiannis
Affiliation:
Lab. of Physical Metallurgy, School of Mining and Metallurgical Engineering, National Technical University of Athens, Athens, Greece
D. Liolios
Affiliation:
Lab. of Physical Metallurgy, School of Mining and Metallurgical Engineering, National Technical University of Athens, Athens, Greece
P. Tsakiridis
Affiliation:
Lab. of Physical Metallurgy, School of Mining and Metallurgical Engineering, National Technical University of Athens, Athens, Greece

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Abstract
Copyright
© Microscopy Society of America 2018 

References

[1] Pike, L. M. Proceedings of the 7th Int. Symposium on Superalloy 718 and Derivatives 2010) p 645.Google Scholar
[2] Joseph, C. Persson, C. M. Hornqvist Colliander. Mater. Sci. Eng. A 679 2017) p. 520.Google Scholar