Surface Analysis of Fine Art Paintings: Studying Degradation Mechanisms with a Systematic Approach

Published online by Cambridge University Press:  01 August 2018

Thomas P Beebe Jr
Affiliation:
University of Delaware, Department of Chemistry & Biochemistry, NewarkDE, USA
Zachary Voras
Affiliation:
University of Delaware, Department of Chemistry & Biochemistry, NewarkDE, USA
Kristin de Gheraldi
Affiliation:
Scientific Analysis of Fine Art LLC & Rijksmuseum, Amsterdam, The Netherlands
Jennifer Mass
Affiliation:
Scientific Analysis of Fine Art LLC & Rijksmuseum, Amsterdam, The Netherlands

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Abstract
Copyright
© Microscopy Society of America 2018 

References

[1] Monico, L., et al, Spectrochimica Acta Part A: Molecular and Biomolecular Spectroscopy 116 2013) p. 270.Google Scholar
[2] Casadio, F., Daher, C. Bellot-Gurlet, L. Top Curr Chem (Z) 374 2016 p.l..Google Scholar
[3] Janssens, K., et al, Top Curr Chem (Z)(374 2016) p. 1.Google Scholar