Super-X XEDS STEM Tomography of y' Precipitates in the LSHR Nickel Superalloy

Published online by Cambridge University Press:  23 September 2015

S.J. Kuhr
Affiliation:
Center for the Accelerated Maturation of Materials, The Ohio State University, Columbus
J.M. Sosa
Affiliation:
Center for the Accelerated Maturation of Materials, The Ohio State University, Columbus
D.E. Huber
Affiliation:
Center for the Accelerated Maturation of Materials, The Ohio State University, Columbus
H.L. Fraser
Affiliation:
Center for the Accelerated Maturation of Materials, The Ohio State University, Columbus

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Abstract
Copyright
Copyright © Microscopy Society of America 2015 

References

References:

[1] Viswanathan, G B, et al., Acta Mater. 53 (2005). pp. 30413057.CrossRefGoogle Scholar
[2] Sarosi, P M, et al., Ultramicroscopy 103 (2005). pp. 8393.Google Scholar
[3] Gayda, J, et al., Superalloys (2004). pp. 323329.CrossRefGoogle Scholar
[4] Uchic, M D, et al., Ultramicroscopy 109 (2009). pp. 12291235.CrossRefGoogle Scholar
[5] Sosa, J M, et al., Integrating Materials and Manufacturing Innovation 3 (2014). p. 18.CrossRefGoogle Scholar