Sintering and Nanoindentation of Ti2SnC (M2AX) Ceramics – Attractive Materials in the Topic of Nuclear Engineering

Published online by Cambridge University Press:  01 August 2018

Snejana Bakardjieva
Affiliation:
Institute of Inorganic Chemistry of the CAS, Husinec - Rez 1001, 250 68 Rez, Czech Republic.
Jiri Vacik
Affiliation:
Nuclear Physics Institute of the CAS, Husinec – Rez 130, 250 68 Rez, Czech Republic.
Jiri Plocek
Affiliation:
Institute of Inorganic Chemistry of the CAS, Husinec - Rez 1001, 250 68 Rez, Czech Republic.
Pavel Horak
Affiliation:
Nuclear Physics Institute of the CAS, Husinec – Rez 130, 250 68 Rez, Czech Republic.
Jiri Nemecek
Affiliation:
Czech Technical University in Prague, Faculty of Civil Engineering, 166 29 Prague, Czech Republic
Robert Klie
Affiliation:
University of Illinois at Chicago, Department of Physics, 845 W Taylor Str., 60 607 Chicago, USA.

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Abstract
Copyright
© Microscopy Society of America 2018 

References

References:

[1] Barsoum, M.W. Prog. Solid State Chem. 28 2000) p. 201.Google Scholar
[2] Shi BoLi, G.P Li, G.P, Bei, H.X., Zhai, Y. Zhou, Mater. Letters 60 2006) p. 3530.Google Scholar
[3] Hu, C, Zhang, H, Li, F, HuAng, Q. Bao, Z. Inter J refract Met and Hard Mater 36 2013) p. 300.Google Scholar
[4] The authors acknowledge funding from the Czech Science Foundation (Project/GACR 18-21677S).Google Scholar