Nanostructure Findings by Use of a Modified Preparation Method of TEM Samples Collected from the Topmost Surface Layer of Carburized Inconel-718 Superalloy

Published online by Cambridge University Press:  01 August 2018

Corneliu Sarbu*
Affiliation:
Independent researcher. Work done at National Institute for Materials Physics, Magurele, Romania

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Abstract
Copyright
© Microscopy Society of America 2018 

References

References:

[1] Collins, S Williams, P Advanced Materials & Processes September 2006) p. 32.Google Scholar
[2] Sharghi-Moshtaghin, R, et al, Metall Mater Trans A 41A 2010) p. 2022.Google Scholar
[3] Williams, P.C Collins, S.R JOM 60(12 2008) p. 27.Google Scholar
[4] Michal, G.M, Ernst, F Heuer, A.H Metall Mater Trans A 37A 2006) p. 1819.Google Scholar
[5] The carburization of IN-718 was done at Swagelok facility. The author is grateful to Swagelok Co. Ltd., Solon, OH and to Dept. of Mater. Sci. & Eng. of Case-Western Reserve Univ., Cleveland, OH for the permission to join the research on surface carburization of IN-718. The financial support of the Romanian Authority ANCSI (Bucharest) for the HR(S)TEM study reported here is acknowledged..Google Scholar