Hostname: page-component-7bb8b95d7b-s9k8s Total loading time: 0 Render date: 2024-10-06T03:38:35.858Z Has data issue: false hasContentIssue false

Multi-Scale Characterization of Different Generations of Gamma Prime Precipitates in Nickel-based Superalloys Using Correlative Microscopy Techniques

Published online by Cambridge University Press:  27 August 2014

T. Rojhirunsakool
Affiliation:
Center for Advanced Research and Technology and Department of Materials Science and Engineering, University of North Texas, Denton, Texas, USA
A.R.P. Singh
Affiliation:
Center for Advanced Research and Technology and Department of Materials Science and Engineering, University of North Texas, Denton, Texas, USA
S. Nag
Affiliation:
Center for Advanced Research and Technology and Department of Materials Science and Engineering, University of North Texas, Denton, Texas, USA
J. Tiley
Affiliation:
Air Force Research Laboratory, Dayton, OH, USA
R. Banerjee
Affiliation:
Center for Advanced Research and Technology and Department of Materials Science and Engineering, University of North Texas, Denton, Texas, USA

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Abstract
Copyright
Copyright © Microscopy Society of America 2014 

References

[1] Singh, A.R.P., Nag, S., Hwang, J.Y., Viswanathan, G.B., Tiley, J., Srinivasan, R., Fraser, H.L., Banerjee, R. Mat. Charac., 62(9), 878 (2011).Google Scholar
[2] Rojhirunsakool, T., Meher, S., Hwang, J.Y., Nag, S., Tiley, J. and Banerjee, R. Jour. Mat. Sci. 48(2), 825 (2013).Google Scholar
[3] Hwang, J.Y., Nag, S., Singh, A.R.P., Srinivasan, R., Tiley, J., Viswanathan, G.B., Fraser, H.L., Banerjee, R. Met. Trans. 40A, 3059-3068 (2009).Google Scholar
[4] Reed, R.C. “The Superalloys: Fundamentals and Applications.” Cambridge University Press, New York (2006).Google Scholar