No CrossRef data available.
Article contents
Microstructural Study of Pt-based Superalloys in the Heat Treated Condition
Published online by Cambridge University Press: 23 November 2012
Abstract
Extended abstract of a paper presented at Microscopy and Microanalysis 2012 in Phoenix, Arizona, USA, July 29 – August 2, 2012.
- Type
- Research Article
- Information
- Microscopy and Microanalysis , Volume 18 , Issue S2: Proceedings of Microscopy & Microanalysis 2012 , July 2012 , pp. 1686 - 1687