Hostname: page-component-586b7cd67f-tf8b9 Total loading time: 0 Render date: 2024-11-28T09:00:48.013Z Has data issue: false hasContentIssue false

Influence of HIP Sintering and Ce/La Additions on the Microstructure and Hardness on Inconel 718 Nickel-based Superalloy

Published online by Cambridge University Press:  30 July 2020

H. M. Medrano-Prieto
Affiliation:
Universidad Autónoma de Ciudad Juárez (UACJ), Ciudad Juárez, Chihuahua, Mexico
C.G. Garay-Reyes
Affiliation:
Centro de Investigación en Materiales Avanzados (CIMAV), Laboratorio Nacional de Nanotecnología, Chihuahua, Chihuahua, México
M.A. Ruiz-Esparza-Rodriguez
Affiliation:
Centro de Investigación en Materiales Avanzados (CIMAV), Laboratorio Nacional de Nanotecnología, Chihuahua, Chihuahua, México
Ivanovich Estrada
Affiliation:
Centro de Investigacion en Materiales Avanzados SC, Chihuahua, Chihuahua, Mexico
J.C. Guía-Tello
Affiliation:
Centro de Investigación en Materiales Avanzados (CIMAV), Laboratorio Nacional de Nanotecnología, Chihuahua, Chihuahua, México
Quirino Estrada
Affiliation:
Universidad Autónoma de Ciudad Juárez (UACJ), Ciudad Juárez, Chihuahua, Mexico
J.M. Silva-Aceves
Affiliation:
Universidad Autónoma de Ciudad Juárez (UACJ), Ciudad Juárez, Chihuahua, Mexico
J.S. Castro-Carmona
Affiliation:
Universidad Autónoma de Ciudad Juárez (UACJ), Ciudad Juárez, Chihuahua, Mexico
H. Camacho-Montes
Affiliation:
Universidad Autónoma de Ciudad Juárez (UACJ), Ciudad Juárez, Chihuahua, Mexico
R. Martínez-Sánchez
Affiliation:
Centro de Investigación en Materiales Avanzados (CIMAV), Laboratorio Nacional de Nanotecnología, Chihuahua, Chihuahua, México

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Collaborative Analysis Using Atom Probe Tomography Including TEM/APT Characterization of Metal Alloys and Other Material Systems
Copyright
Copyright © Microscopy Society of America 2020

References

Bassinia, E., Vola, V., Lorusso, M., Ghisleni, R., Lombardi, M., Biamino, S., Ugues, D., Vallillo, G., Picqué, B., Mater. Sci. Eng. A, 695 (2017) p. 5565.10.1016/j.msea.2017.04.016CrossRefGoogle Scholar
Chen, Ming-Song, Zou, Zong-Huai, Lin, Y.C., Li, Hong-Bin, Wang, Guan-Qiang, Ma, Yan-Yong, Mater. Charact, 151 (2019) p. 445456.10.1016/j.matchar.2019.03.037CrossRefGoogle Scholar
Appa Rao, G., Srinivas, M., Sarma, D.S., Mater. Sci. Eng. A, 418 (2006) p. 282-291.Google Scholar
Baskaran, T., Arya, Shashi Bhushan, Ceram. Int, 44 (2018) p. 17695-17708.10.1016/j.ceramint.2018.06.234CrossRefGoogle Scholar