HAADF Imaging and MD Simulations of Microtwining Partial Dislocations in Nickel Based Superalloy Rene 104,

Published online by Cambridge University Press:  03 August 2008

L Kovarik
Affiliation:
The Ohio State University
RR Unocic
Affiliation:
The Ohio State University
J Li
Affiliation:
University of Pennsylvania
MJ Mills
Affiliation:
The Ohio State University
Get access

Extract

Extended abstract of a paper presented at Microscopy and Microanalysis 2008 in Albuquerque, New Mexico, USA, August 3 – August 7, 2008