Evaluation of low temperature degradation of 3Y-TZP in artificial saliva

Published online by Cambridge University Press:  25 July 2016

María del Carmen Aragón Duarte
Affiliation:
Departamento de Física, Centro de Investigation en Materiales Avanzados S.C. (CIMAV), Miguel de Cervantes 120, Complejo Industrial, C.P. 31109, Chihuahua, México
Armando Reyes Rojas
Affiliation:
Departamento de Física, Centro de Investigation en Materiales Avanzados S.C. (CIMAV), Miguel de Cervantes 120, Complejo Industrial, C.P. 31109, Chihuahua, México
Hilda E. Esparza-Ponce
Affiliation:
Departamento de Física, Centro de Investigation en Materiales Avanzados S.C. (CIMAV), Miguel de Cervantes 120, Complejo Industrial, C.P. 31109, Chihuahua, México

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Abstract
Copyright
© Microscopy Society of America 2016 

References

References:

[1] Manicone, PF, Iommeti, PR & Raffaelli, L Journal of Dentistry 35 (2007). pp. 819826.Google Scholar
[2] Deville, S, Gremillard, L, Gerome, C & Gilbert, F Journal of Biomedical Materials Research Part B: Applied Biomaterials 72B (2005). pp. 239245.Google Scholar
[3] ISO 13356 Implants for surgery — Ceramic materials based on yttria-stabilized tetragonal zirconia (Y-TZP).Google Scholar