Effect on Microstructure and Nanoindentation of a AlCoFeMoNi High Entropy Alloy.

Published online by Cambridge University Press:  01 August 2018

F.J. Baldenebro-Lopez
Affiliation:
FIM-Universidad Autónoma de Sinaloa, Los Mochis, Sinaloa, México.
C.D. Gómez-Esparza
Affiliation:
Centro de Investigación en Materiales Avanzados (CIMAV), Chihuahua, Chih
H. Camacho-Montes
Affiliation:
FIM-Universidad Autónoma de Sinaloa, Los Mochis, Sinaloa, México.
R. Martínez-Sánchez
Affiliation:
IIT-Universidad Autónoma de Ciudad Juárez., Ciudad Juárez, Chih., México.

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Abstract
Copyright
© Microscopy Society of America 2018 

References

References:

[1] Chen, Y.L., et al, Alloys Compd 477 2008) p. 696.Google Scholar
[2] Shun, T.T., Du, Y.C. Compd, J. Alloys 479 2009) p. 157.Google Scholar