Hostname: page-component-586b7cd67f-r5fsc Total loading time: 0 Render date: 2024-11-24T11:55:20.442Z Has data issue: false hasContentIssue false

Effect of Heavy Mass Ion (Gold) and Light Mass Ion (Boron) Irradiation on Microstructure of Tungsten

Published online by Cambridge University Press:  28 May 2019

Prashant Sharma*
Affiliation:
ITER-India, Institute for Plasma Research, Bhat, Gandhinagar 382428, India
Padivattathumana Maya
Affiliation:
ITER-India, Institute for Plasma Research, Bhat, Gandhinagar 382428, India
Satyaprasad Akkireddy
Affiliation:
Institute for Plasma Research, Bhat, Gandhinagar 382428, India
Prakash M. Raole
Affiliation:
ITER-India, Institute for Plasma Research, Bhat, Gandhinagar 382428, India
Anil K. Tyagi
Affiliation:
ITER-India, Institute for Plasma Research, Bhat, Gandhinagar 382428, India Homi Bhabha National Institute, Training School Complex, Anushaktinagar, Mumbai 400094, India
Asha Attri
Affiliation:
ITER-India, Institute for Plasma Research, Bhat, Gandhinagar 382428, India
Pawan K. Kulriya
Affiliation:
Inter-University Accelerator Centre Aruna Asaf Ali Marg, New Delhi 110067, India
Parmendra K. Bajpai
Affiliation:
Guru Ghasidas Vishwavidyalaya, Koni, Bilaspur 495009, India
Sudhir Mishra
Affiliation:
Bhabha Atomic Research Centre, Mumbai 400 085, India
Shiv P. Patel
Affiliation:
Guru Ghasidas Vishwavidyalaya, Koni, Bilaspur 495009, India
Tarkeshwar Trivedi
Affiliation:
Guru Ghasidas Vishwavidyalaya, Koni, Bilaspur 495009, India
K. B. Khan
Affiliation:
Bhabha Atomic Research Centre, Mumbai 400 085, India
Shishir P. Deshpande
Affiliation:
ITER-India, Institute for Plasma Research, Bhat, Gandhinagar 382428, India Homi Bhabha National Institute, Training School Complex, Anushaktinagar, Mumbai 400094, India
*
*Author for correspondence: Prashant Sharma, E-mail: [email protected], [email protected]
Get access

Abstract

The difference in the defect structures produced by different ion masses in a tungsten lattice is investigated using 80 MeV Au7+ ions and 10 MeV B3+ ions. The details of the defects produced by ions in recrystallized tungsten foil samples are studied using transmission electron microscopy. Dislocations of type b = 1/2[111] and [001] were observed in the analysis. While highly energetic gold ion produced small clusters of defects with very few dislocation lines, boron has produced large and sparse clusters with numerous dislocation lines. The difference in the defect structures could be due to the difference in separation between primary knock-on atoms produced by gold and boron ions.

Type
Materials Applications
Copyright
Copyright © Microscopy Society of America 2019 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

Chou, YT (1972). Dislocation reactions and networks in anisotropic b.c.c. crystals. Mater. Sci. Eng. C 100, 8186. doi: 10.1016/0025-5416(72)90071-7.Google Scholar
Federici, G, Biel, W, Gilbert, MR, Kemp, R, Taylor, N & Wenninger, R (2017). European DEMO design strategy and consequences for materials ITER conceptual design. Nucl Fusion 570(092002), 125. doi: 10.1088/1741-4326/57/9/092002.Google Scholar
Grzonka, J, Ciupiński, L, Smalc-Koziorowska, OV, Ogorodnikova, M, Mayer, KJ & Kurzydłowski, (2014). Electron microscopy observations of radiation damage in irradiated and annealed tungsten. Nucl. Instr. Meth. Phys. Res. B 340, 2733. 10.1016/j.nimb.2014.07.043.Google Scholar
Hasanzadeh, S, Schäublin, R, Décamps, B, Rousson, V, Autissier, E, Barthe, MF & Hébert, C (2018). Three-dimensional scanning transmission electron microscopy of dislocation loops in tungsten. Micron 1130(May), 2433. doi: 10.1016/j.micron.2018.05.010.Google Scholar
Hideo, W, Naoki, F, Shiori, N & Naoaki, Y (2014). Microstructure and thermal desorption of deuterium in heavy-ion-irradiated pure tungsten. J Nucl Mater 4550(1–3), 5155. doi: 10.1016/j.jnucmat.2014.03.060.Google Scholar
Hull, D & Bacon, JD (2011). Introduction to Dislocations, vol. 1. 5th ed. Oxford, UK: Butterworth-Heinemann, Elsevier Ltd. 10.1016/B978-0-08-096672-4.00006-2.Google Scholar
Kanjilal, D, Chopra, S, Narayanan, MM, Iyer, IS, Vandana, J, Joshi, R & Datta, SK (1993). Testing and operation of the 15UD Pelletron at NSC. Nucl. Instr. Meth. Phys. Res. A 3280(1–2), 97100. doi: 10.1016/0168-9002(93)90610-T.Google Scholar
Kaufmann, M & Neu, R (2007). Tungsten as first wall material in fusion devices. Fusion Eng Des 820(5–14), 521527. doi: 10.1016/j.fusengdes.2007.03.045.Google Scholar
Kinchin, GH & Pease, RS (1955). The displacement of atoms in solids by radiation. Rep Prog Phys 180(1), 151. doi: 10.1088/0034-4885/18/1/301.Google Scholar
Labelle, AJ-RR (2011). The Effects of Helium on Deuterium Retention in Tungsten Under Simultaneous Irradiation. Thesis, University of Toronto.Google Scholar
Lassner, E & Schubert, WD (2012). Tungsten: properties, chemistry, technology of the element, alloys, and chemical compounds. USA: Springer. ISBN 9781461549079.Google Scholar
Nandipati, G, Setyawan, W, Heinisch, HL, Roche, KJ, Kurtz, RJ & Wirth, BD (2015). Displacement cascades and defect annealing in tungsten, part III: The sensitivity of cascade annealing in tungsten to the values of kinetic parameters. J Nucl Mater 462, 345353. doi: 10.1016/j.jnucmat.2015.01.059.Google Scholar
Norfleet, DM, Dimiduk, DM, Polasik, SJ, Uchic, MD & Mills, MJ (2008). Dislocation structures and their relationship to strength in deformed nickel microcrystals. Acta Mater 560(13), 29883001. doi: 10.1016/j.actamat.2008.02.046.Google Scholar
Ogorodnikova, OV, Gasparyan, Y, Efimov, V, Ciupinski, L & Grzonka, J (2014). Annealing of radiation-induced damage in tungsten under and after irradiation with 20 MeV self-ions. J Nucl Mater 4510(1), 379386. ISSN.Google Scholar
Oya, Y, Li, X, Sato, M, Yuyama, K, Zhang, L, Kondo, S, Hinoki, T, Hatano, Y, Watanabe, H, Yoshida, N & Chikada, T (2015). Thermal desorption behavior of deuterium for 6 MeV Fe ion irradiated W with various damage concentrations. J Nucl Mater 461, 336340. doi: 10.1016/j.jnucmat.2015.03.032.Google Scholar
Pitts, RA, Carpentier, S, Escourbiac, F, Hirai, T, Komarov, V, Lisgo, S, Kukushkin, AS, Loarte, A, Merola, M, Sashala Naik, A, Mitteau, R, Sugihara, M, Bazylev, B & Stangeby, PC (2013). A full tungsten divertor for ITER: Physics issues and design status. J Nucl Mater 4380(Suppl), S48S56. doi: 10.1016/j.jnucmat.2013.01.008.Google Scholar
Roth, J, Tsitrone, E, Loarte, A, Loarer, T, Counsell, G, Neu, R, Philipps, V, Brezinsek, S, Lehnen, M, Coad, P, Grisolia, C, Schmid, K, Krieger, K, Kallenbach, A, Lipschultz, B, Doerner, R, Causey, R, Alimov, V, Shu, W, Ogorodnikova, O, Kirschner, A, Federici, G & Kukushkin, A (2009). Recent analysis of key plasma wall interactions issues for ITER. J Nucl Mater 390–3910(1), 19. doi: 10.1016/j.jnucmat.2009.01.037.Google Scholar
Rueden, CT, Johannes, S, Hiner, MC, DeZonia, BE, Walter, AE, Arena, ET & Eliceiri, KW (2017). Imagej2: Imagej for the next generation of scientific image data. BMC Bioinformatics 180(1), 529. doi: 10.1186/s12859-017-1934-z.Google Scholar
Taylor, N, Merrill, B, Cadwallader, L, Di Pace, L, El-Guebaly, L, Humrickhouse, P, Pinna, T, Panayotov, D, Reyes, S, Porfiri, M-T, Shimada, M & Willms, S (2017). Materials-related issues in the safety and licensing of nuclear fusion facilities ITER conceptual design recent citations. Nucl Fusion 570(092003), 128.Google Scholar
Trivedi, T, Patel Shiv, P, Chandra, P & Bajpai, PK (2017). Ion beam facilities at the national centre for accelerator based research using a 3 MV Pelletron accelerator. Phys Procedia 900(November), 100106. doi: 10.1016/j.phpro.2017.09.032.Google Scholar
Was, GS (2007). Fundamentals of Radiation Materials Science, vol. 44. Berlin, Heidelberg, New York: Springer. ISBN 9788578110796. doi: 10.1017/CBO9781107415324.004.Google Scholar
Was, GS & Andresen, PL (2014). Woodhead Publishing Series in Energy. Cambridge, UK: Woodhead Publishing. pp. 355420. 10.1533/9780857097552.2.355.Google Scholar
Yao, B, Edwards, DJ & Kurtz, RJ (2013). TEM characterization of dislocation loops in irradiated bcc Fe-based steels. J Nucl Mater 4340(1–3), 402410. doi: 10.1016/j.jnucmat.2012.12.002.Google Scholar
Yi, X, Jenkins, ML, Kirk, MA, Zhou, Z & Roberts, SG (2016). In-situ TEM studies of 150 keV W+ ion irradiated W and W-alloys: Damage production and microstructural evolution. Acta Mater 112, 105120. doi: 10.1016/j.actamat.2016.03.051.Google Scholar
Ziegler, JF (1988). The stopping and range of ions in solids. In Ion Implantation Science and Technology, Ziegler, JF (Ed.), 2nd ed.Ed. pp. 361. London, UK: Academic Press 10.1016/B978-0-12-780621-1.50005-8.Google Scholar
Ziegler, JF, Ziegler, MD & Biersack, JP (2010). SRIM—The stopping and range of ions in matter (2010). Nucl. Instr. Meth. Phys. Res. B 2680(11–12), 18181823. doi: 10.1016/j.nimb.2010.02.091.Google Scholar