Discontinuous Precipitation in Aged Welded Joints of High Cr-Ni Superalloy

Published online by Cambridge University Press:  04 August 2017

J.C. Spadotto
Affiliation:
Department of Chemical and Materials Engineering, PUC-Rio, Rio de Janeiro, Brazil
I.G. Solorzano
Affiliation:
Department of Chemical and Materials Engineering, PUC-Rio, Rio de Janeiro, Brazil

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Abstract
Copyright
© Microscopy Society of America 2017 

References

[1] Guan, K., et al, Nucl. Eng. Des 235(23 2005). p. 2485.Google Scholar
[2] Manna, I., et al, Int. Mater. Rev 46(2 2001). p. 53.Google Scholar
[3] The authors acknowledge are grateful to CBPF for the access to the LabNano Electron Microscopy facilities and to the Brazilian Funding agencies CAPES and CNPq.Google Scholar