Deformation of Borides in Nickel-based Superalloys: a Study of Segregation at Dislocations

Published online by Cambridge University Press:  05 August 2019

Lola Lilensten*
Affiliation:
Max-Planck-Institut für Eisenforschung, Max-Planck Strasse 1, 40237 Düsseldorf, Germany
Stoichko Antonov
Affiliation:
Illinois Institute of Technology, 10 W. 32nd Street, Chicago, IL, 60616, USA Beijing Advanced Innovation Center for Materials Genome Engineering, State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083, China
Dierk Raabe
Affiliation:
Max-Planck-Institut für Eisenforschung, Max-Planck Strasse 1, 40237 Düsseldorf, Germany
Sammy Tin
Affiliation:
Illinois Institute of Technology, 10 W. 32nd Street, Chicago, IL, 60616, USA
Baptiste Gault
Affiliation:
Max-Planck-Institut für Eisenforschung, Max-Planck Strasse 1, 40237 Düsseldorf, Germany Department of Materials, Imperial College, South Kensington, London SW7 2AZ, UK
Paraskevas Kontis
Affiliation:
Max-Planck-Institut für Eisenforschung, Max-Planck Strasse 1, 40237 Düsseldorf, Germany
*
*Corresponding author: [email protected]

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
New Frontiers in Atom Probe Tomography Applications
Copyright
Copyright © Microscopy Society of America 2019 

References

[1]Tytko, D, Choi, P, Klöwer, J, Kostka, A, Inden, G, Raabe, D, Acta Materialia 60 (2012), p. 1731.Google Scholar
[2]Kontis, P, Yusof, HAM, Pedrazzini, S, Danaie, M, Moore, KL, Bagot, PAJ, Moody, MP, Grovenor, CRM, Reed, RC, Acta Materialia 103 (2016), p. 688.Google Scholar
[3]Hamadi, S, Hamon, F, Delautre, J, Cormier, J, Villechaise, P, Utada, S, Kontis, P, Bozzolo, N, Metallurgical and Materials Transaction A 49 (2018), p. 4246.Google Scholar
[4]Kontis, P, Li, Z, Collins, DM, Cormier, J, Raabe, D, Gault, B, Scripta Materialia 145 (2018), p. 76.Google Scholar
[5]Wu, X, Makineni, SK, Kontis, P, Dehm, G, Raabe, D, Gault, B, Eggeler, G, Materialia 4 (2018), p. 109.Google Scholar
[6]The authors thank Rolls Royce Corporation and Siemens Turbomachinery AB for providing the RRHT3 and STAL15-CC superalloys, respectively.Google Scholar