Contribution of the Microfractography on the Study of Mechanical Properties of Alloys.

Published online by Cambridge University Press:  28 April 2020

Carlos Lariot*
Affiliation:
Institute of Science and Technology of Materials (IMRE-UH) Havana, Cuba
Amalek Orellana
Affiliation:
Institute of Science and Technology of Materials (IMRE-UH) Havana, Cuba
Xenia Suárez
Affiliation:
Laboratory of Tropicalization Assays (LABET) Havana, Cuba

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Abstract
Copyright
Copyright © Microscopy Society of America 2020

References

References:

[1]Orellana, A.Tesis Maestría. Universidad de La Habana, 2014.Google Scholar
[2]Suárez, Xenia, Acosta, Lisbet, Corvo, Francisco, Lariot, Carlos. MEMORIAS de Convención Internacional CUBA INDUSTRIA. Taller Tropicalización. ISBN 978-959-282-097-5, 3770-3777, 2014Google Scholar