Microstructure and Microanalysis of Ni-based Superalloy Exhaust Valves

Published online by Cambridge University Press:  01 August 2004

N. D. Evans
Affiliation:
Oak Ridge National Laboratory, Oak Ridge, Tennessee
P. J. Maziasz
Affiliation:
Oak Ridge National Laboratory, Oak Ridge, Tennessee
L. R. Walker
Affiliation:
Oak Ridge National Laboratory, Oak Ridge, Tennessee
Get access

Extract

Extended abstract of a paper presented at Microscopy and Microanalysis 2004 in Savannah, Georgia, USA, August 1–5, 2004.