The Effects of Cooling Rate on the Microstructure of a Commercial Ni-based Superalloy Using Atom Probe Tomography

Published online by Cambridge University Press:  05 August 2007

PM Sarosi
Affiliation:
The Ohio State University
MK Miller
Affiliation:
Oak Ridge National Laboratory
D Isheim
Affiliation:
Northwestern University
M Mills
Affiliation:
The Ohio State University
Get access

Extract

Extended abstract of a paper presented at Microscopy and Microanalysis 2007 in Ft. Lauderdale, Florida, USA, August 5 – August 9, 2007