Combined AFM Nanoindentation and Finite Element Analysis of Soft Heterogeneous Biomaterials

Published online by Cambridge University Press:  23 November 2012

B.L. Doss
Affiliation:
Department of Physics, Arizona State University, Tempe, AZ
J.R. Staunton
Affiliation:
Department of Physics, Arizona State University, Tempe, AZ
M. Dannemeyer
Affiliation:
Department of Physics, Arizona State University, Tempe, AZ
M. Linhart
Affiliation:
Department of Physics, Arizona State University, Tempe, AZ
R. Ros
Affiliation:
Department of Physics, Arizona State University, Tempe, AZ
Get access

Abstract

Extended abstract of a paper presented at Microscopy and Microanalysis 2012 in Phoenix, Arizona, USA, July 29 – August 2, 2012.