Hostname: page-component-586b7cd67f-2plfb Total loading time: 0 Render date: 2024-11-29T07:44:06.397Z Has data issue: false hasContentIssue false

Characterization of Niobia Deposited via Atomic Layer Deposition on Mesoporous Silica for Improved Hydrothermal Stability

Published online by Cambridge University Press:  23 November 2012

H. Pham
Affiliation:
Chemical & Nuclear Engineering, University of New Mexico, Albuquerque, NM
A. Anderson
Affiliation:
Chemical & Nuclear Engineering, University of New Mexico, Albuquerque, NM
A. Datye
Affiliation:
Chemical & Nuclear Engineering, University of New Mexico, Albuquerque, NM
Y. Pagan-Torres
Affiliation:
University of Wisconsin-Madison, Madison, WI
J. Dumesic
Affiliation:
University of Wisconsin-Madison, Madison, WI
Get access

Abstract

Extended abstract of a paper presented at Microscopy and Microanalysis 2012 in Phoenix, Arizona, USA, July 29 – August 2, 2012.